The creation and characterisation of biodegradable blend films based on chitosan and polyvinyl alcohol for application in a range of packaging is described. The compatibility between the chitosan and PVA polymers was good. Composite films had a compact and homogeneous structure, according to the morphology analysis. The mechanical test result of PVA/CH at concentrations 5% showed, that The higher values of TS recorded in sample (p1, with 40 MPa) while the lower values appeared in sample (p9, with 22.09 MPa), the TS decreased gradually as the amount of PVA increased in blend film. While the blend film of pure Chitosan exhibits a poor mechanical strength which makes it a poor candidate for packaging but Blending CH with PVA together improved tensile strength. PVA/CH at concentrations 10%. Showed the higher TS values appeared in sample (C1 with 36.64MPa) while the lower values of TS appeared in sample (C9 with 24.4 MPa). In comparison with pure PVA have the lower TS than all blend film. The result of mechanical properties after addition of borax solution revealed that the Borax improves the E at max and TS of blend films. Mechanical properties results of CH/PVA/Tio2, Showed that the TS and E at max were increased after introducing of Tio2 into the polymer matrix. The P1 sample have been chosen according to their possess acceptable TS, E at max to be subjected to gamma radiation at different doses 2.3, 3.5, 4.5, 6, 7.5 kGy. The results demonstrated, that the increasing the radiation doses lead to increasing in TS of blend film, following increasing in E at max, the highest TS of the irradiated films is observed at 7.5.kGy dose.
In this experimental study, the use of stone powder as a stabilizer to the clayey soil studied. Tests of Atterberg limits, compaction, fall cone (FCT), Laboratory vane shear (LVT), and expansion index (EI) were carried out on soil-stone powder mixtures with fixed ratios of stone powder (0%, 5%, 10%, 15%, and 20%) by the dry weight. Results indicated that the undrained shear strength obtained from FCT and LVT increased at all the admixture ratios, and the expansion index reduced with the increase of the stone powder.
Background: The geriatric patients wearing removable partial dentures are increasing in proportion. At the same time, the root caries prevalence accompanied by gingival recession is increasing. A variety of vehicles can deliver fluoride into the oral cavity, including fluoride mouth-rinse, fluoride dentifrice, topical fluoride, and fluoride-releasing restorative materials, all of which effectively prevent root caries and suppress recurrent caries. This study aimed to evaluate the effect of sodium fluoride addition on some mechanical properties of heat cure acrylic denture base material. Material and method: A total of 90 samples were prepared in this study, then divided into three main groups according to the type of test used (hardness, te
... Show MoreThe determination of critical micelle concentration of selected non-ionic surfactants (Tween 20,40 and 80) have been investigated using magnetic water(MW)as an aqueous medium.Conductometry technique is used to determine critical micelle concentration.The effect of alcohol addition and temperature variation at the range(293.15 -303.15K) are also pursued. It is concluded that the process of micellization is spontaneous and endothermic because of the observed free energy of micellization (ΔGom) , enthalpy change of micellization (ΔHom), and entropy change of micellization (ΔSom) for the system was also studied.The properties of the non-ionic surfactants were studied, both in absence and presence of
... Show MoreThe acrylic polymer composites in this study are made up of various weight ratios of cement or silica nanoparticles (1, 3, 5, and 10 wt%) using the casting method. The effects of doping ratio/type on mechanical, dielectric, thermal, and hydrophobic properties were investigated. Acrylic polymer composites containing 5 wt% cement or silica nanoparticles had the lowest abrasion wear rates and the highest shore-D hardness and impact strength. The increase in the inclusion of cement or silica nanoparticles enhanced surface roughness, water contact angle (WCA), and thermal insulation. Acrylic/cement composites demonstrated higher mechanical, electrical, and thermal insulation properties than acrylic/silica composites because of their lowe
... Show MoreThe work was carried out in two stages. The first stage concerned
with study of silicon carbide (SiC) ratio (1.5, 2.5, 3.5, and 4.5 wt%)
effect on the Thermal conductivity of polyvinyl chloride (PVC); and
the second stage concerned with the UV – weatherizing (25, 50, and
75 hr), thermal aging (40, 50, and 60 °C), and rain- weatherizing (1,
2.5, and 4 hr) effect on the samples involved. Thermal conductivity
results proved that there was slight increase in thermal conductivity
by (SiC) loading; it increased from 0.17 W/m.K for PVC to 0.19
W/m.K for 4.5% SiC/PVC; where as it was systematically decreased
by UV- weatherizing, thermal aging, and rain- weatherizing. This
property is in a good agreement with gene
The research was conducted in one of the fields of the Department of Plant Production in the desert region (tomato development project) affiliated with the Directorate of Agriculture of the Holy Karbala Governorate for the purpose of studying the effect of spraying the shoots of the Kohlrabi plant (hybrid) with the Nano biopolymer (Chitosan) and the Azotobacter bio inoculum on the roots of the plant seedlings in terms of growth indicators and yield for the autumn agricultural season. 2023-2024 ,The means were compared according to the Duncan multiple ranges test at significant to level of 0.05.with R.C.B.D . The first factor was spraying the shoots with Nano- Chitosan at a concentration of (0, 1, and 2) g L-1, two weeks after transplanting,
... Show MoreThis study was conducted to test the effect of aqueous and alcoholic extracts for cyperus rotundus on the mitosis in tap roots of Allium cepa. the result of general an identical qualitative tests showed contains certain compounds that of crude aqueous and alcoholic extract, Used as five different concentrations of (10, 20.38, 56, 75) mg / ml for a period of four hours of treatment. After the chemical has been detected for some preliminary chemical compounds of the crude aqueous extract, while the alcoholic extract either phenol compound has been detected for phenols using several techniques included the use of thin layer chromatography TLC and measurement of disability factor RF and the degree of fusion and measurement of absorbance. The r