Preferred Language
Articles
/
HRYYo4oBVTCNdQwCbaId
Investigating the optical and electrical characteristics of As60Cu40-xSex thin films
...Show More Authors

In this work, As60Cu40-xSex thin films were synthesized, and the pulsed laser deposition method was used to study the effected partial replacement of copper with selenium. The electrical characteristics and optical characteristics, as indicated by the absorbance and transmittance as a function of wavelength were calculated. Additionally, the energy gap was computed. The electrical conductivity of the DC in the various conduction zones was calculated by measuring the current and voltage as a function of temperature. Additionally, the mathematical equations are used to compute the energy constants, electron hopping distance, tail width, pre-exponential factor, and density of the energy states in variation zones (densities of the energetic extended states N(Eext), localize N(Eloc) and at the Fermi states N(Ef)). The acquired data also demonstrated that the selenium concentration obviously had an impact on the electrical conduction mechanics, energy states, and the level of randomization.

Scopus Clarivate Crossref
View Publication
Publication Date
Thu May 11 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Effect Annealing Temperatures On The Structural Proerties of ZnO Thin Films Prepared By Chemical Bath Deposition
...Show More Authors

In this research, we study the changing structural properties of ZnO with changing annealing temp., in the range  (473-773)K prepared by chemical bath deposition method at temp. (353)K, where deposited on glasses substrates at thickness (500±25)nm, the investigation of (XRD) indicates that the (ZnO) films are polycrystalline type of Hexagonal.

            The results of the measuring of each sample from grain size, microstrain, dislocation density, integral breadth, shape factor and texture coefficient, show that annealing process leads to increase the grain size (26.74-57.96)nm, and decrease microstrain (0.130-0.01478), dislocation density (1.398-0.297)*1015

... Show More
View Publication Preview PDF
Publication Date
Sat Jul 01 2023
Journal Name
Journal Of Materials Science: Materials In Electronics
Effect of phosphoric acid chemical etching on morphological, structural, electrical, and optical properties of porous GaAs Schottky diodes
...Show More Authors

View Publication
Scopus (6)
Crossref (4)
Scopus Clarivate Crossref
Publication Date
Sat Jan 05 2019
Journal Name
Iraqi Journal Of Physics
Study the structural and optical properties of titanium oxide thin film, doped with chromium prepared in Sol-Gel method
...Show More Authors

This paper presents the effect of Cr doping on the optical and structural properties of TiO2 films synthesized by sol-gel and deposited by the dip- coating technique. The characteristics of pure and Cr-doped TiO2 were studied by absorption and X-ray diffraction measurement. The spectrum of UV absorption of TiO2 chromium concentrations indicates a red shift; therefore, the energy gap decreases with increased doping. The minimum value of energy gap (2.5 eV) is found at concentration of 4 %. XRD measurements show that the anatase phase is shown for all thin films. Surface morphology measurement by atomic force microscope (AFM) showed that the roughness of thin films decrease with doping and has a minimum value with 4 wt % doping ratio.

View Publication Preview PDF
Crossref (3)
Crossref
Publication Date
Wed Jun 01 2022
Journal Name
Iraqi Journal Of Physics
Synthesis and Characterization of Ternary BexZn1-xO Nano Thin Films prepared by Pulsed Laser Deposition Technique
...Show More Authors

         Beryllium Zinc Oxide (BexZn1-xO) ternary nano thin films were deposited using the pulsed laser deposition (PLD) technique under a vacuum condition of 10-3 torr at room temperature on glass substrates with different films thicknesses, (300, 600 and 900 nm). UV-Vis spectra study found the optical band gap for Be0.2Zn0.8O to be  (3.42, 3.51 and 3.65 eV) for the (300, 600 and 900nm) film thicknesses, respectively which is larger than the value of zinc oxide ZnO (3.36eV) and smaller than that of beryllium oxide BeO (10.6eV). While the X-ray diffraction (XRD) pattern analysis of ZnO, BeO and Be 0.2 Zn 0.8 O powder and nano-thin films indicated a hexa

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Wed Jul 17 2024
Journal Name
Journal Of Optics
Influence of concentration on optical and structural properties of zinc sulfide films using spray pyrolysis technique
...Show More Authors

View Publication
Scopus Clarivate Crossref
Publication Date
Wed Jan 01 2020
Journal Name
International Conference Of Numerical Analysis And Applied Mathematics Icnaam 2019
Synthesis of nanostructure diamond-like carbon thin films by atmospheric pressure plasma jet
...Show More Authors

In this work, diamond-like carbon (DLC) thin films were prepared from Cyclohexane. Thin films were deposited on quartz substrate by atmospheric pressure Argon plasma jet system. The plasma jet system was applying high voltage sinusoidal waves of frequency 28 kHz and potential difference of 7.5kV peak to peak across the electrodes. The effect of annealing at 400, 500 and 600 °C under vacuum for two hours on optical properties and structural properties of the DLC thin films were investigated. This effect was clarified by X-ray diffraction (XRD), FTIR, UV-Visible absorption, Scanning Electron Microscopy (SEM) and Raman Spectroscopy. The X-ray diffraction patterns for the annealing DLC thin films show two broad peaks at 2θ, 26.62° and 51.58

... Show More
View Publication
Scopus (2)
Crossref (2)
Scopus Clarivate Crossref
Publication Date
Mon Aug 03 2020
Journal Name
Digest Journal Of Nanomaterials And Biostructures
PREPARATION OF MIXED In2O3 – CdO THIN FILMS BY CSP TECHNIQUE FOR LIGHT SENSING
...Show More Authors

In this work, chemical spray pyrolysis deposition (CSP) technique was used to prepare a mixed In2O3-CdO thin films with different CdO content (10, 30 and 50)%volume ratio on glass substrates at 150 ᵒC substrate temperature. The surface morphology and structural properties were measured to find the optimum conditions to improve thin films properties for using as photo detector. Current –Time, the sensitivity and response speed vary for each mixture. Samples with 10% vol. CdO content has square pulse response with average rise time nearly 1s and fall time 1s.

Publication Date
Thu Mar 01 2018
Journal Name
Materials Today Communications
Improved mechanical properties of sol-gel derived ITO thin films via Ag doping
...Show More Authors

View Publication
Scopus (19)
Crossref (21)
Scopus Clarivate Crossref
Publication Date
Mon Feb 18 2019
Journal Name
Iraqi Journal Of Physics
Studying the spectral properties of thin films of rhodamine (6G) dyes doped polymer (PMMA) dissolved in chloroform
...Show More Authors

              In the present work, poly methyl methacrylate (PMMA) doped with Rhodamine 6G was prepared. The spectral properties (absorption and fluorescence) of the films were studied at different concentrations (1x10-5, 2x10-5, 5x10-5, 7x10-5, and 1x10-4mol/l). The investigated samples were made in the form of thin films. This was achieved by dissolving a certain weight of PMMA in a fixed volume of chloroform, composite films was with thickness (25.8μm) at room temperature. The achieved results were pointed out that absorption and fluorescence spectra have taken a wide spectral rang so when increased the concentratio

... Show More
View Publication Preview PDF
Crossref
Publication Date
Sun Aug 06 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Study of Optical Properties of CdS Films Prepared by Thermal Evaporation in Vacuum
...Show More Authors

CdS films were prepared by thermal evaporation at pressure (10-6torr) of 1μm thickness onto glass substrate by using (Mo) boat. The optical properties of CdS films, absorbance, transmittance and reflectance were studied in wavelength range of (300-900)nm. The refractive index, extinction coefficient, and absorption coefficient were also studied. It's found that CdS films have allowed direct and forbidden transition with energy gap 2.4eV and 2.25eV respectively and it also has high absorption coefficient (α >104cm-1).

View Publication Preview PDF