Aim: To evaluate the commercial pure titanium disks that structuring by laser in two design (dot and groove) each one with three different laser scan (5, 15 and 25) and comparing with titanium surface that not subjected to any surface structuring (control) through measuring the wettability test and surface roughness test. Materials and methods: Structuring on the surface of the commercial pure titanium (CP Ti) disks was performed via using fiber laser CNC machine in two design (dot and groove) in three different laser scans (5, 15 and 25), then the structuring disks analyzed with the control group by atomic force microscope and water contact angle test. Results: The results of this study showed that the surface roughness and the wettability of commercial pure titanium disks for the dot and groove structuring design increased with the increasing of the laser scans. The result also show that laser structuring with dot design for any laser scan showed higher wettability and roughness values when compared to the groove design for the same laser scans. Conclusion: The surface roughness and the wettability of the CP Ti disks increased when dot and groove design laser surface structuring were applied to the CP Ti disks especially at 25 laser scans.
In this work, the nano particles of Na-A zeolite were synthesized by sol –gel method. The samples were characterized by X-ray diffraction (XRD), X-ray luorescence (XRF), Surface area and pore volume, Atomic Force Microscope (AFM) and Fourier Transform Infrared Spectroscopy (FTIR). Results show that the nano A zeolite is with average crystal size is 74.77 nm., Si/Al ratio 1.03, BET surface area was 581.211m2/g and the pore volume for NaA was found equal to 0.355cm3/g.
Two methods have been applied for the spectrophotometric determination of atropine, in
bulk sample and in dosage form. The methods are accurate, simple, rapid, inexpensive and
sensitive. The first method depending on the extraction of the formed ion-pair complex with
bromphenol blue (BPB) as a chromogenic reagent in chloroform, use phthalate buffer of pH
3.0; which showed absorbance maxima at 413 nm against reagent blank. The calibration
graph is linear in the ranges of 0.5-40 µg.mL
-1
with detection limit of 0.363µg.mL
-1
. The
second method depending on the measure of the absorbance maxima of the formed charge-transfer complex with 2,3-dichloro-5,6-dicyano-p-benzoquinone (DDQ) at 457 nm against
The aim of the present research is concerned with study the effect of UV radiation on the optical properties at wavelengths 254, 365 nm of pure PC and anthracene doping PC films prepared using the cast method for different doping ratio 10-60 mL. Films of pure PC and anthracene doping PC were aged under UV radiation for periods of up to 360 h. It found that the effect of UV radiation at wavelength 254 nm on the optical properties is great than the effect of UV radiation at wavelength 365 nm. Also, it found that the optical energy gap of pure PC and anthracene doping PC films is stable against radiation.
The primary function of commercial banks is the process of converting liquid liabilities such as deposits to illiquid assets, (also known as a loan), liquid assets, (aka cash and cash equivalent) in a balanced manner between liquid and illiquid assets, that guaranteed the preservation of the rights of depositors and the bank and not by converting liquid liabilities into liquid assets in a very large percentage. This comes from its role as depository and intermediary institutions between supply and demand, therefore, we find that the high indicators of bank liquidity and solvency may reflect a misleading picture of the status of commercial banks, to some extent in terms of the strength of their balance sheets and
... Show MoreThe study involved the removal of acidity from free fatty acid via the esterification reaction of oleic acid with ethanol. The reaction was done in a batch reactor using commercial 13X zeolite as a catalyst. The effects of temperatures (40 to 70 °C) and reaction time (up to 120 minutes) were studied using 6:1 mole ratio of pure ethanol to oleic acid and 5 wt. % of the catalyst. The results showed that acid removed increased with increasing temperature and reaction time. Also, the acidity removal rises sharply during the first reaction period and then changes slightly afterward. The highest acidity removal value was 67 % recorded at 110 minutes and 70 °C. An apparent homogeneous reversible reaction kinetic model has been proposed a
... Show MoreHeavy metal (HM) pollution has long been a significant source of environmental deterioration and a problem for the safety of food. Iraqis prefer rice over any other food, and since heavy metals have a direct impact on health, their traces in rice have drawn particular attention. Before cooking rice, it is usual in Iraq to wash and soak it. Some 55 varieties of imported and local rice were sampled from Erbil city markets in 2022 with the aim of determining the concentration of As, Cd, Cr, Ni and Pb before and after soaking. Standard procedure of acid digestions was applied on the raw and soaked samples. The solutions were analyzed using ICPE-9820 Shimadzu. The mean concentrations of As, Cd, Cr, Ni and Pb (in mg/kg) in the rice samples bef
... Show MoreThis paper presents the effect of Cr doping on the optical and structural properties of TiO2 films synthesized by sol-gel and deposited by the dip- coating technique. The characteristics of pure and Cr-doped TiO2 were studied by absorption and X-ray diffraction measurement. The spectrum of UV absorption of TiO2 chromium concentrations indicates a red shift; therefore, the energy gap decreases with increased doping. The minimum value of energy gap (2.5 eV) is found at concentration of 4 %. XRD measurements show that the anatase phase is shown for all thin films. Surface morphology measurement by atomic force microscope (AFM) showed that the roughness of thin films decrease with doping and has a minimum value with 4 wt % doping ratio.
Objective This study evaluated the effects of adding titanium oxide (TiO2) nanofillers on the tear strength, tensile strength, elongation percentage, and hardness of room-temperature-vulcanized (RTV) VST50F and high-temperature-vulcanized (HTV) Cosmesil M511 maxillofacial silicone elastomers. Methods Two types of maxillofacial elastomers, VST50F RTV and Cosmesil M511 HTV, were used. Nano-TiO2 powder was applied as a nanofiller. A total of 120 specimens were fabricated, 60 each of VST50F and Cosmesil M511. The specimens of each type of elastomer were divided into three equal groups on which tests were conducted for tear strength, tensile strength, and hardness i.e., 20 specimens were used for each test. Each group of 20 specimens was further
... Show More