This paper presents experimental investigations on buried Glass Reinforced Plastic (GRP) pipes with a diameter of 1400 mm. The tested pipes were buried in dense, gravelly sand and subjected to traffic loads to study the effects of backfill cover on pipe deflection. The experimental program included tests on three GRP pipes with backfill covers of 100 cm, 75 cm, and 50 cm. The maximum traffic loads applied to the pipe–soil system corresponded to Iraqi Truck Type 3 (AASHTO H type). Vertical deflections of the pipes were monitored during the application of these loads. The experimental results showed that, as the backfill cover increased, the maximum vertical deflection of the pipe decreased. Deflection reductions were 38.0% and 33.3% when the backfill increased from 50 cm to 100 cm and from 50 cm to 75 cm, respectively. A 500 mm compacted backfill cover was found to be sufficient to resist traffic loads, with the vertical deflection percentage remaining below the allowable limit. Additionally, the behavior of the GRP pipes under different traffic load configurations was analyzed using finite element (FE) analysis with Plaxis 3D. The model was validated using field data. The study investigated numerous variables impacting the behavior of embedded pipes, including pipe material, pipe thickness, backfill properties, backfill depth, and the properties of the soil beneath the GRP pipe. The deflections of the steel pipe were lower than those of the GRP pipe when using different thicknesses.
The reinforced fiberglass in cement slurry reflects the effect on its properties compared to usual additives. Fiberglass is typically used in cement slurry design for one or another of the following goals: (Earth earthquake, bearing storage, and with differential stresses, to enhance cement durability and increase its compressive strength). The main goal is to use glass fiber and ground fiberglass to improve the tensile strength and moderate compressive strength significantly. On the other hand, the use of glass fibers led to a slight increase in the value of thickening time, which is a desirable effect. Eleven glass fiber samples and milled glass fiber were used to show these materials' effect on Iraqi cement with (0.125, 0.25, 0.5
... Show MoreCultivation of the green seaweed Enteromorpha compressa was performed under natural laboratory spring environmental conditions of temperature, light intensity and photoperiod to study the salinity tolerance of this intertidal green macroalga. Cultivation was carried out under artificial seawater (ASW) of different concentrations (18, 35, 53 and 106 g/l sea salt) compared to the control using natural seawater (NSW). Growth rate and pigment content of the cultivated alga were recorded at regular intervals during the experimental duration. Antioxidant activity of the crude ethanolic extract and its fractions (petroleum ether, chloroform, ethyl acetate and acetone) was performed against DPPH radical scavenging assay and compared to
... Show MoreBackground: White spot lesions (WSLs) are subsurface enamel demineralization manifested as white opacities which had an esthetic problem. The purpose of this in-vitro study was to evaluate the lesion depth improvement of WSLs following application of fluoride varnish, tooth mousse and resin infiltration (ICON). Materials and methods: Artificial WSLs were created on 120 premolar teeth using demineralization solution with pH (4-4.5). Samples randomly allocated into four groups; fluoride varnish, tooth mousse, ICON and untreated group. Groups were discolored in Cola and orange juice for 24 hours. Teeth were ground sectioned by longitudinal cutting then these sections examined and photographed under stereomicroscope at 12X magnification then an
... Show MoreThe ceramic compound Mg1-xSixAl2O4 (x= 0, 0.1, 0.2, 0.3, 0.4) was prepared from nano powder of Al2O3 and MgO doped with Nano powder of SiO2 at different molar ratios. The specimens were prepared by standard chemical solid reaction technique and sintered at 1450 oC. Structure of the specimens was analyzed by using X-ray diffraction (XRD). The X-ray patterns of the specimens showed the formation of pure simple cubic spinel structure MgAl2O4 phase with space group of ̅ . The average grain size and surface topology were studied by atomic force microscopy. The results showed that the average grain size was about 73-90 nm. The DC electrical properties of the specimen were measured. The apparent density was found to increase and the porosity a
... Show MoreEffect of nano and micro SiO2 particles with different weight percent (2,4,6,8 and 10) %wt on the Interlaminar fracture toughness (GIc) of 16-plies of woven roving glass fiber /epoxy composites prepared by hand lay – up technique were investigated. The specimens were tested using DCB test (mode I).
Area method was used to compute the interlaminar fracture toughness. The results show that, GIc would increase with the increasing in the filler content, the main failure in microcomposites and nanocomposites was delamination in the layers, the delamination reduced with increasing in the filler content.
Oil is considered the most important source for providing the funds for the national economic sectors. The revenues of oil constitute %95 of the GPD. Therefore, the development of the remaining sectors depend on oil..
The Iraqi Oil Marketing Organization (SOMO) depended on the a unified price for all the buyers, That may not reflect the real value of market and did not contribute in marketing the type of heavy oil. Then, to what extent had SOMO been able to market the light and heavy crude oil in a way that contains the expected increase in the crude oil production.
Phoenix dactylifera l. pinnae (the green leaves of dates palm) were used as natural reinforcing (strengthening) fibers to improve the mechanical properties of polyester as a matrix material, the fibers of the green leaves of dates palm were used in two lengths, 10 and 20mm with five rates of 0, 2.5, 5, 10, and 20% , where the reinforcing with the leaves fibers increases the hardness strength from 76.5 to be about 86.55 , the Impact value raised from about 0.313 to 0.461 , in addition to that the flexural strength from 2.66 to be about 55 , and the thermal conductivity increases from 2.54 𝑤∕𝑚.℃ to 5.41 𝑤∕𝑚.℃. The results of the present search explains that the composite samples reinforced at rate 20% and 10mm fiber length
... Show More