Background: The bond strength of the root canal sealers to dentin is very important property for maintaining the integrity and the seal of root canal filling. The aim of this study was to evaluate and compare the push-out bond strength of root filled with total fill Bioceramic, AH Plus and Gutta-flow®2 sealers using GuttaFusion®obturation system versus single cone obturation technique. Materials and method: sixty of mandibular premolars teeth with straight roots were used in this study, these roots were instrumented using Reciproc system, instrumentation were done with copious irrigation of 3 mL 5.25% sodium hypochlorite solution (NaOCl) during all the steps of preparation, and smear layer will be removed with 1 ml of 17% EDTA kept in the canal for 1 min, roots were randomly divided into two groups according to the obturation technique (thirty teeth for each group): Group I: Single Reciproc Gutta percha cone obturation technique, Group II: Gutta fusion obturation technique, then each group divided into three subgroup according to the type of sealer, AH subgroup: AH Plus sealer, BC subgroup: bioceramic sealer and GF subgroup: Gutta flow 2 sealer. The roots then stored in moist environment at 37°C for one week, the roots were embedded in clear acrylic resin and each root sectioned into three levels apical, middle and cervical. The bond strength was measured using computerized universal testing machine each section fixed in the machine so that the load applied from apical to cervical direction at 0.5mm/min. speed and the computer show the higher bond force before dislodgment of the filling material. These forces were divided by the surface area to obtain the bond strength in MPa. Results: Statistical analysis was performed and the result showed a highly significant differences between the three types of sealers when the same obturation technique were used, also there is highly significant differences between two groups with two different obturation technique. Conclusion: This study showed that the push out bond strength of AH plus sealer was higher than bioceramic sealer and Gutta flow 2 sealer respectively when the same obturation technique was used. The push out bond strength was affected by the obturation technique and Gutta fusion obturation technique showed higher bond strength than single cone obturation technique when the same type of sealer was used.
The first aim of this paper was to evaluate the push-out bond strength of the gutta-percha coating of Thermafil and GuttaCore and compare it with that of gutta-percha used to coat an experimental hydroxyapatite/polyethylene (HA/PE) obturator. The second aim was to assess the thickness of gutta-percha around the carriers of GuttaCore and HA/PE obturators using microcomputed tomography (
Background: Reduction in bond strength when bonding was done immediately after intracoronal bleaching procedure has been recognized. The purpose of this study is to assess the effect of antioxidants (10% sodium ascorbate (SA), 0.1M thiourea and7% sodium bicarbonate (SB)) on reversing bonding strength of composite resin to bleached dentin. Materials and method: Sixty upper 1st premolar teeth, were selected, the crowns of the teeth were embedded in acrylic resin blocks exposing a flat dentin from the buccal surface, then divided into 6 groups (10 samples each). Bleaching for the experimental groups was performed using 35% hydrogen peroxide bleaching gel (pola–office).Group A (Negative
... Show MoreABSTRACT Background: Bracket rebonding is a common problem in orthodontics which may result in many drawbacks. The aims of this study were to evaluate the effects of application of two enamel protective agents “Icon†and “ProSeal†on shear bond strength before and after rebonding of stainless steel orthodontic brackets using conventional orthodontic adhesive and to assess the site of bond failure. Materials and methods: Fifty sound extracted human upper first premolar teeth were selected and randomly divided into two equal groups; the first time bonding and the rebonding groups (n=30). Each group was subdivided into control, Icon and ProSeal subgroups. The enamel protective agents were applied after etching (precondi
... Show MoreBackground: In this study we evaluate the effect of plasma treatment (oxygen and argon) gas in two different exposure times on the surface of heat cure and light cure acrylic resin. Materials and method: 100 specimens of heat cure and light cure acrylic resin were fabricated. The measurements of the samples were (75mm, 25mm and 4.5mm) length, width and depth respectively with stopper of 3mm depth. Two types of gas used oxygen and argon in (5,10) min by using (DC-glow discharge plasma device) then we apply cold cure soft lining material, with the help of Instron machine we test the shear stress value. Results: A highly significant effect after argon and oxygen gases treatment in both 5 and 10 min exposure times on shear bond strength to soft
... Show More
Purpose: To evaluate the effect of different surface treatments on shear bond strength between dentin and IPS e.max lithium disilicate glass-ceramic. Materials and Methods: Eighteen extracted third molars were embeded in epoxy resin. The tooth was sectioned vertically in mesiodistal direction using a low speed hard tissue microtome. The buccal and lingual surfaces of each section were ground flat using 600 grit Silicone carbide paper. Eighteen ceramic discs consisted of lithium disilicate glass-ceramic were prepared with a diameter of 4.7mm and height of 2.2mm. The discs were divided in two groups (n=10): (1) IPS e.max treated with hydrofluoric acid and Monobond Plus (MBP) and (2) IPS e.max treated with Monobond Etch &Prime (MBEP). The toot
... Show MoreBackground: This study was aimed to investigate the effect of three lingual button (Nickel free / rectangular base, Nickel free / round base and Composite) and bonding environment, wet and dry enamel surface, on: the shear bond strength (SBS) of light and self-cured Resin Modified Glass Ionomer Cements, and the debonding failure sites. Materials and method: One hundred twenty no-carious, free of cracks maxillary first premolar teeth were selected. Three types of orthodontic lingual buttons were used in this study: Nickel free / rectangular base, Nickel free / round base and Composite buttons. The teeth were divided into two groups of sixty teeth each. One group was used for testing the chemically cured GC Fuji Ortho Resin modified Glass Io
... Show More