Indium oxide In2O3 thin films fabricated using thermal evaporation of indium metal in vacuum on a glass substrate at 25oC using array mask, after deposition the indium films have been subjected to thermal oxidation at temperature 400 °C for 1h. The results of prepared Indium oxide reveal the oxidation method as a strong effect on the morphology and optical properties of the samples as fabricated. The band gap (Eg) of In2O3 films at 400 °C is 2.7 eV. Then, SEM and XRD measurements are also used to investigate the morphology and structure of the indium oxide In2O3 thin films. The antimicrobial activity of indium oxide In2O3 thin films was assessed against gram-negative bacterium using inhibition zone of bacteria which improved higher ina
... Show MoreNano-crystalline iron oxide nanoparticles (magnetite) was synthesized by open vessel ageing process. The iron chloride solution was prepared by mixing deionized water and iron chloride tetrahydrate. The product was characterized by X-Ray, Surface area and pore volume by Brunauer-Emmet-Teller, Atomic Force Microscope (AFM) and Fourier Transform Infrared Spectroscopy(FTIR) . The results showed that the XRD in compatibility of the prepared iron oxide (magnetite) with the general structure of standard iron oxide, and in Fourier Transform Infrared Spectroscopy, it is strong crests in 586 bands, because of the expansion vibration manner related to the metal oxygen absorption band (Fe–O bonds in the crystals of iron ox
... Show MoreIn this study, Zinc oxide nanostructures were synthesized via a hydrothermal method by using zinc nitrate hexahydrate and sodium hydroxide as a precursor. Three different annealing temperatures were used to study their effect on ZnO NSs properties. The synthesized nanostructure was characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), Atomic force microscope (AFM), and Fourier Transform Infrared Spectroscopy (FTIR). Their optical properties were studied by using UV -visible spectroscopy. The XRD analysis confirms that all ZnO nanostructures have the hexagonal wurtzite structure with average crystallite size within the range of (30.59 - 34
... Show MoreIn this study, aluminum nanoparticles (Al NPs) were prepared using explosive strips method in double-distilled deionized water (DDDW), where the effect of five different currents (25, 50, 75, 100 and 125 A) on particle size and distribution was studied. Also, the explosive strips method was used to decorate zinc oxide particles with Al particles, where Al particles were prepared in suspended from zinc oxide with DDDW. Transmission electron microscopy (TEM), UV-visible absorption spectroscopy, and x-ray diffraction are used to characterize the nanoparticles. XRD pattern were examined for three samples of aluminum particles and DDDW prepared with three current values (25, 75 and 125 A) and three samples prepared with the same currents for zin
... Show MoreA competitive adsorption of Cu2+, Ni2+, and Cd2+ ions from a synthetic wastewater onto nanomaterial was studied.(Fe3O4) nanoparticles obtained from US Research Nanomaterials, Inc., Houston, TX 77084, (USA), was used as nanosorbent. Experimental parameters included pH, initial metal concentrations, and temperature were studied for nanosorbent. The uptake capacity 11.5, 6.07 and 11.1 mg/g for Cu2+, Ni2+and Cd2+, respectively, onto nanosorbent . The optimum pH values was 6 and the contact time was 50 min. for Cu2+, Ni2+and Cd2+, respectively. The equilibrium isotherm for
... Show MoreFunctionalized-multi wall carbon nanotubes (F-MWCNTs) and functionalized-single wall carbon nanotubes (F-SWCNTs) were well enhanced using CoO Nanoparticles. The sensor device consisted of a film of sensitive material (F-MWCNTs/CoONPs) and (F-SWCNTs/CoO NPs) deposited by drop- casting on an n-type porous silicon substrate. The two sensors perform high sensitivity to NO2 gas at room temperatures. The analysis indicated that the (F-MWCNTs/CoONPs) have a better performance than (F-SWCNTs/CoONPs). The F-SWCNTs/CoONPs gas sensor shows high sensitivity (19.1 %) at RT with response time 17 sec, while F-MWCNTs/CoONPs gas sensor show better sensitivity (39 %) at RT with response time 13 sec. The device shows a very reproducible sensor p
... Show MoreAbstract The surface of kaolin was diagnosed by an AFM and the results were shown The height of the highest peak reached by a quantity of Kaolin surface is 2.5 µm, the granules, and their diameter with an average diameter of 666.1nm. Using Kaolin's adsorption properties, erythrosine was removed of its aqueous solution. It was determined that the maximal dye adsorption ranged 36.53–40.61%. The results of using the Freundlich, Langmuir, and Temkin adsorption isotherms revealed that at temperatures of (298,308,318) K, the Freundlich model was followed, the Langmuir model did not match, and the Temkin model could only be partially applied. There is also physical adsorption. One of the three kinetic models of the
... Show More
ABSTRACT
A field experiment was carried out in the fields of the college of agricultural engineering sciences, university of Baghdad during the fall season of 2021, in order to find out which of the cultivated genotypes of maize are efficient under nitrogen fertilization. The experiment was applied according to a RCBD (split plot design with three replications). The genotypes of experiment (Baghdad, 5018 and Sarah) and supplying three levels of nitrogen fertilizer, which are N1 (100 kg/ha), N2 (200 kg/ha) and N3 (300 kg/ha), the results of the statistical analysis are showed the superiority of the cultivar Sarah in the trait of number of days until 50% silking, chlorophyll
... Show MoreThis work describes the synthesis of novel ligand (H2L2) (4-((2-hydroxy-5-nitrophenyl)imino)methyl)-5(hydroxymethyl)-2methylpyridin-3-ol) type (NOO) donor atoms. When it coordinates with metal ions[V2+,Mn2+,Fe2+,Co2+,Ni2+,Cu2+and Pt4+] with the general formula K2[M(L2)2].XH2O and K2[VO(L2)(OSO3)].H2O . This ligand can form tridentate structures. The ligand was synthesized from the reaction of pyridoxal hydrochloride with 2-amino-4-nitrophenol in ethanol (as a solvent) at a mole ratio of 1:1 and thoroughly mixed and refluxed for 6-8 hrs . The reaction