Rutting has a significant impact on the pavements' performance. Rutting depth is often used as a parameter to assess the quality of pavements. The Asphalt Institute (AI) design method prescribes a maximum allowable rutting depth of 13mm, whereas the AASHTO design method stipulates a critical serviceability index of 2.5 which is equivalent to an average rutting depth of 15mm. In this research, static and repeated compression tests were performed to evaluate the permanent strain based on (1) the relationship between mix properties (asphalt content and type), and (2) testing temperature. The results indicated that the accumulated plastic strain was higher during the repeated load test than that during the static load tests. Notably, temperature played a major role. The power-law model was used to describe the relationship between the accumulated permanent strain and the number of load repetitions. Furthermore, graphical analysis was performed using VESYS 5W to predict the rut depth for the asphalt concrete layer. The α and µ parameters affected the predicted rut depth significantly. The results show a substantial difference between the two tests, indicating that the repeated load test is more adequate, useful, and accurate when compared with the static load test for the evaluation of the rut depth.
The aim of this research work is to study the effect of stabilizing gypseous soil, which covers vast areas in the middle, west and south parts of Iraq, using liquid asphalt on its strength properties to be used as a base course layer replacing the traditional materials of coarse aggregate and broken stones which are scarce at economical prices and hauling distances. Gypseous soil brought from Al-Ramadi City, west of Iraq, with gypsum content of 66.65%, medium curing cutback asphalt (MC-30), and hydrated lime are used in this study. The conducted tests on untreated and treated gypseous soil with different percentages of medium curing cutback asphalt (MC-30), water, and lime were: unconfined compression strength, and one dimensional confine
... Show MoreMoisture induced damage in asphaltic pavement might be considered as a serious defect that contributed to growth other distresses such as permanent deformation and fatigue cracking. This paper work aimed through an experimental effort to assess the behaviour of asphaltic mixtures that fabricated by incorporating several dosages of carbon fiber in regard to the resistance potential of harmful effect of moisture in pavement. Laboratory tests were performed on specimens containing fiber with different lengths and contents. These tests are: Marshall Test, the indirect tensile test and the index of retained strength. The optimum asphalt contents were determined based on the Marshall method. The preparation of asphaltic mixtures involved
... Show MoreFor over a century, the global consumption of asphalt binder in asphalt mixture production has been substantial. In the Heet region (west of Iraq), two distinct forms of natural asphalt (NA) deposits exist: rock asphalt and sulfur spring asphalt. This study focused on using NA sourced from sulfur springs. The aim was to investigate the potential of incorporating NA into local asphalt mixtures. To achieve this, NA was heated to 163°C for varying durations. After heat treatment, laboratory tests were conducted on NA. The findings suggest that by heating NA for 20 hours, it conforms to Iraqi specifications in terms of physical properties. Furthermore, compared to conventional petroleum asphalt, treated NA showed greater
... Show MoreGypseous soil is considered as a problematic soil for embankment construction, however, implementation of emulsified asphalt as a stabilization agent could be a proper solution for enhancing its properties as a subgrade soil. In this work, the sustainability of asphalt stabilized soil has been assessed in terms of its resistance to cyclic (freezing-thawing) and (heating-cooling) processes. Specimens have been prepared at optimum fluid content (moisture and emulsion) and tested under direct shear stresses while subjected to 30 cycles of (freezing-thawing) and (heating-cooling). Both of dry and soaked testing conditions have been implemented. Data have been observed after each 10 cycles, and compared with that of reference mix. It was conclud
... Show MoreWarm Mix Asphalt (WMA) is a modern energy-saving process that uses environmentally friendly materials, has lower mixing and compaction temperatures, and uses less energy and releases less contaminants than conventional hot mix asphalt. Moisture damage poses one of the main challenges of the material design in asphalt pavements. During its design life, the asphalt pavement is exposed to the effect of moisture from the surrounding environment. This research intends to investigate the role of the polypropylene fibres for modifying the moisture susceptibility for the WMA by using different percentages of polypropylene (namely 2, 4, and 6%) by weight of the binder of the control mixture (WMA). In this paper, the physical characteristics
... Show MoreThis work investigates generating of pure phase Faujasite-type zeolite Y at the ranges chosen for this study via a static aging step in the absence of seeds synthesis. Nano-sized crystals may result when LUDOX AS-40 is used as a silica source for gel composition of range 6 and the crystallization step may be conducted for a period of 4 to 19 hr at 100 ⁰C. Moreover, large-crystals with high crystallinity pure phase Y zeolite can be obtained at hereinabove conditions but when hydrous sodium metasilicate is used as a silica source. The other selected ranges also offer pure phase Y zeolite at the same controlled conditions.
This work investigates generating of pure phase Faujasite-type zeolite Y at the ranges chosen for this study via a static aging step in the absence of seeds synthesis. Nano-sized crystals may result when LUDOX AS-40 is used as a silica source for gel composition of range 6 and the crystallization step may be conducted for a period of 4 to 19 hr at 100 ⁰C. Moreover, large-crystals with high crystallinity pure phase Y zeolite can be obtained at hereinabove conditions but when hydrous sodium metasilicate is used as a silica source. The other selected ranges also offer pure phase Y zeolite at the same controlled conditions.
Technique was used to retail for analyzing atom beryllium ion cathode of an atom lithium to six pairs of functions wave which two ?????? and the rest of the casing moderation and to analyze atom lithium ion Mob atom beryllium to three pairs of functions wave pair of casing and the rest of the casing moderation using function wave Hartree Fock and each casing email wascalculate expected values ??....
This study investigated the structural behavior of a beam–slab member fabricated using a steel C-Purlins beam carrying a profile steel sheet slab covered by a dry board sheet filled with recycled aggregate concrete, called a CBPDS member. This concept was developed to reduce the cost and self-weight of the composite beam–slab system; it replaces the hot-rolled steel I-beam with a steel C-Purlins section, which is easier to fabricate and weighs less. For this purpose, six full-scale CBPDS specimens were tested under four-point static bending. This study investigated the effect of using double C-Purlins beams face-to-face as connected or separated sections and the effect of using concrete material that contains different recycled
... Show More