Background: This in vitro study compares a self-etch primer (SEP) to an etch-and-rinse (EaR) for bonding sapphire brackets by evaluation of the enamel etch-pattern, shear bond strength, amount of remnant adhesive and enamel surface damage following thermal and fatigue cyclic loading. Material and Methods: Ceramic (sapphire) brackets were bonded to 80 extracted human premolars using two enamel etching protocols: conventional EaR using 37% phosphoric acid (PA) gel (control), and a SEP (Transbond Plus). Each group was subdivided into two subgroups (n=20 teeth) according to the time of bracket debonding: after 24 h water storage or following 5000 thermo-cycles plus 5000 cycles fatigue loading, to determine the shear bond strength (SBS), adhesive remnant index (ARI score), with scanning electron microscopy (SEM) evaluation of enamel condition. Results: The control subgroups consistently exhibited significantly higher (p ˂ 0.05) SBS mean values (23.4-29.8 MPa) than the SEP subgroups (15.1-22.4 MPa) at both bracket debonding time points. However, the SEP subgroups yielded milder etch-patterns and attained SBS values above the minimum requirement range for clinical performance. In addition, the higher SBS of control subgroups was accompanied with higher ARI scores and enamel damage grades than SEP subgroups as confirmed by SEM. Thermocycling and fatigue significantly reduced the SBS of all subgroups, with a non-significant drop in the amount of adhesive residue or enamel damage. Conclusions: The use of SEP can be a suitable alternative to the conventional PA gel for sapphire bracket bonding as it maintains suitable bond strength and has the potential to produce both less remnant adhesive and enamel damage
Background: The use of Miswak, chewing sticks (salvadorapersica) can be traced back to Babylonians some 7000 years ago. It is commonly used throughout the world especially for the purpose of oral hygiene. Muslims are using as the religious view. Current study aimed to test the ability of aqueous siwak extract to increase the resistance of enamel surface against acid dissolution compared to sodium fluoride. Materials and Method: Twenty maxillary first premolars were treated with the selected solutions included two aqueous siwak extract concentration(5%,10%) and sodium fluoride(0.05%)as control positive for 2 minutes once daily for 20days interval, de ionized water was used as control negative. The concentration of the dissolved phosphorus i
... Show MoreBackground: Debonding and fracture of artificial teeth from denture bases are common clinical problem, bonding of artificial teeth to heat cure acrylic and high impact heat cure acrylic denture base materials with autoclave processing method is not well known. The aim of this study was to evaluate the effect of autoclave processing method on shear bond of artificial teeth to heat cure denture base material and high impact heat cure denture base material. Materials and methods: Heat polymerized (Vertex) and high impact acrylic (Vertex) acrylic resins were used. Teeth were processed to each of the denture base materials after the application of different surface treatments. The sample (which consist of artificial tooth attached to the dentur
... Show MoreThis study deals with the aircraft wing analysis (numerical and experimental) which subjected to fatigue loading in order to analyze the aircraft wing numerically by using ANSYS 15.0 software and experimentally by using loading programs which effect on fatigue test specimens at laboratory to estimate life of used metal (aluminum alloy 7075-T651) the wing metal and compare between numerical and experimental work, as well as to formulate an experimental mathematical model which may find safe estimate for metals and most common alloys that are used to build aircraft wing at certain conditions. In experimental work, a (34) specimen of (aluminum alloy 7075-T651) were tested using alternating bending fatigue machine rig. The t
... Show MoreBackground: This study aimed to evaluate the effect of zirconia different surface treatments (primer, sandblast with 50μmAl2O3, Er,Cr:YSGG laser) on shear bond strength between zirconia surface and resin cement. Material and methods: Sixty presintered Y-TZP zirconia cylinder specimens (IPS e.max ZirCAD, Ivoclar vivadent) will be fabricated and sintered in high temperature furnace of (1500 C for 8 hours) according to manufacturer’s instructions to the selected size and shape of (5mm. in diameter and 6mm in height). All specimens were ground flat using 600.800.1000.1200, aluminum oxide abrasive paper to obtain a standardized surface roughness. Surface roughness values were then recorded in µm using surface roughness tester (profi
... Show MoreAbstract: Fluoroquinolones drugs are an important class of wide
... Show MoreThe present work covers the analytical design process of three dimensional (3-D) hip joint prosthesis with numerical fatigue stress analysis. The analytical generation equations describing the different stem constructive parts (ball, neck, tour, cone, lower ball) have been presented to reform the stem model in a mathematical feature. The generated surface has been introduced to FE solver (Ansys version 11) in order to simulate the induced dynamic stresses and investigate the effect of every design parameter (ball radius, angle of neck, radius of neck, neck ratio, main tour radius, and outer tour radius) on the max. equivalent stresses for hip prosthesis made from titanium alloy. The dynamic loading case has been studied to a stumbling ca
... Show MoreObjective: To identify of the effect of the different concentrations of the special liquid (for mixing the investment, Gilvest)
and mixed with water/powder ratio on setting time of phosphate–bonded investment.
Method and materials: The present study is (60) specimens made from phosphate bonded investment divided into (4)
groups (control and experimental groups), (15) specimens for each group. The Gillmore needle device is used to setting
time of phosphate bonded investment mixed with different concentration of Gilvest and water.
Results: Showed that there is a high significant difference (P<0.01) between each groups in the ANOVA test and a
significant difference (P<0.05) between the group (A) and control group i