Denture base materials made using three-dimensional printing (3D printing) have expanded in availability, contributing to the meteoric rise of this innovative dental technique. Despite 3D-printed denture resins having good biocompatibility and esthetics, achieving superior mechanics in these materials is still difficult. This study aimed to find out how adding calcium carbonate (CaCO
3
) nanoparticles to 3D-printed denture base resin affected its surface hardness, impact strength, and flexural strength. The ninety 3D printed samples were allocated into three groups following the amount of CaCO
3
NPs added to the resin: one control group had no CaCO
3
, and two modified groups—one had 1.5 wt.%, and the other group had 2 wt.%. Surface hardness, impact, and flexural strength were the three test specifications used to further divide each group into three subgroups. Analysis was also conducted utilizing energy dispersive X-ray spectroscopy (EDX) and field emission scanning electron microscopy (FESEM). All data were statistically analyzed. The results verified that adding CaCO
3
NPs to the 3D-printed denture resin significantly boosted its impact strength, flexural, and surface hardness (
The reaction of LAs-Cl8 : [ (2,2- (1-(3,4-bis(carboxylicdichloromethoxy)-5-oxo-2,5- dihydrofuran-2-yl)ethane – 1,2-diyl)bis(2,2-dichloroacetic acid)]with sodium azide in ethanol with drops of distilled water has been investigated . The new product L-AZ :(3Z ,5Z,8Z)-2- azido-8-[azido(3Z,5Z)-2-azido-2,6-bis(azidocarbonyl)-8,9-dihydro-2H-1,7-dioxa-3,4,5- triazonine-9-yl]methyl]-9-[(1-azido-1-hydroxy)methyl]-2H-1,7-dioxa-3,4,5-triazonine – 2,6 – dicarbonylazide was isolated and characterized by elemental analysis (C.H.N) , 1H-NMR , Mass spectrum and Fourier transform infrared spectrophotometer (FT-IR) . The reaction of the L-AZ withM+n: [ ( VO(II) , Cr(III) ,Mn(II) , Co(II) , Ni(II) , Cu(II) , Zn(II) , Cd(II) and Hg(II)] has been i
... Show More