The increasing requirement and use of dental implant treatments has rendered dental implantology indispensable in dentistry. The aim of this study is to determine the optimum concentration of calcium silicate to be incorporated into a polyetherketoneketone (PEKK) matrix used as an implant material to enhance the bioactivity and mechanical properties of the composite compared with unmodified PEKK. In this study, different weight percentage (wt%) of micro-calcium silicate (m-CS) is incorporated into PEKK with ethanol as a binder. Subsequently, the mixture is dried in a forced convection oven at 120°C and poured into customized molds to fabricate a bioactive composite via compression molding (310°C, 15 MPa, and 20 min holding time) ( n = 5). The mechanical properties and in vitro apatite-forming ability of the composites are investigated. Although an apatite layer is formed on all composites after immersion in simulated body fluid for 7 days, the flexural strength and elastic modulus of the composite increased after the filler load is increased to 15 wt%, whereas it decreased in groups with filler loadings exceeding 15 wt%. The results of this study indicate that the incorporation of 15 wt% m-CS into the PEKK polymeric matrix can improve the bioactivity and mechanical properties of this bioactive composite.
A new series of morpholine derivative were prepared by reacting the morpholine with ethyl chloro acetate in the presence triethylamine as an catalyst and benzene as a solvent gave the ethyl morpholin-4-ylacetate reaction with hydrazine hydrate and ethanol as a solvent gave the 2-(morpholin-4-yl)acetohydrazide gave series of Schiff base were prepared by reacting 2-(morpholin-4- yl)acetohydrazide with different aromatic aldehydes and ketons . The new series of (3-9 )were synthesis by reaction of Schiff base (10-14) with chloroacetyl chloride, triethyl amine as an catalyst and 1,4dioxane as a solvent .The chemical structures of the synthesis compound were identified by spectral methods their [ IR ,1H-NMR and 13C-NMR ].The synthesised compoun
... Show MoreNanosponges (NS) of etodolac(ETO) was prepared using the emulsion solvent diffusion method ; the effects of drug: polymer ratio, the effect of level concentration of internal phase and stirring time and other variables that effect on the physical characteristics of NS were investigated and characterized, The selected formula was lyophilized then incorporated into hydrogel ; which also evaluated .The results show that the formulation that contain Drug: PVA:EC in ratio 1:3:2 is the best with smallest particle size 40.2±0.098 with polydispersibility0.005 and in vitro release 97.6±0.11%, , ETO NS Carbopol hydrogel produced a significant(p<0.05) improvement of the in vitro release than pure ETO hydrogel.
The presence of alkaloids in Crassula ovata is a topic that is still unexplored, as there are no published studies on the matter. This study demonstrates the presence of an alkaloid compound (and its class) for the first time in Crassula ovata. The plant material was defatted with n-hexane, and a Soxhlet apparatus was used for the extraction process, while the acid-base method was used for the isolation of alkaloids from the chloroform fractions. The quaternary alkaloid was precipitated from the aqueous layer spontaneously, in high quantity. By using standard spectroscopic methods (including liquid chromatography - mass spectroscopy) we were able to clarify the structure of the precipi¬tated compound as a tetrahydroprotoberberine a
... Show MoreIn present project, new Schiff base of 4, 4'- (((1E, 1'E)-1,4-.phenylenebis- (methane-ylylidene))-bis-(azane-ylylidene)) bis-(5-(4-chlorophenyl) -4H -1,2,4-triazole-3-thione) (L3) has been synthesized by condensation of 4-amino-5-(4-chlorophenyl)-2,4-dihydro-3H-1,2,4-triazole-3-thione with benzene-1,4-dicarboxaldehyde. The new asymmetrical Schiff base (L3) used as a ligand to synthesize a new complex with Co(II), Ni(II), Cu(II), Pd(II), and Pt(IV) metal ions by 1:2 (Metal: ligand) ratio. New ligand and their complexes have been exanimated and Confirmed by Fourier-transform infrared (FT-IR), Ultraviolet-visible (UV-visible), Proton nuclear magnetic resonance (1HNMR), carbon13 nuclear magnetic resonance (13CNMR), carbon-hydrogen nitrogen sulf
... Show MoreIn this research prepared two composite materials , the first prepared from unsaturated polyester resin (UP) , which is a matrix , and aluminum oxide (Al2O3) , and the second prepared from unsaturated polyester resin and aluminum oxide and copper oxide (CuO) , the two composites materials (Alone and Hybrid) of percentage weight (5,10,15)% . All samples were prepared by hand layup process, and study the electrical and thermal conductivity. The results showed decrease electrical conductivity from (10 - 2.39) ×10-15 for (Up+ Al2O3) and from (10 - 2.06)×10-15 for (Up+ Al2O3+ CuO) .But increase thermal conductivity from( 0.17 - 0.505) for (Up+ Al2O3) and from (0.17 - 0.489) for (Up+ Al2O3+ CuO).
Background: Endodontically treated teeth have low resistance to fracture against occlusal forces. The strengthening effect of bonded esthetic onlay restoration on weakened tooth has been reported. This study aimed to assess the fracture resistance of endodontically treated premolars restored with composite with and without cuspal coverage by using direct and indirect techniques. Indirect technique done by CAD/CAM system (computer aided design –computer aided manufacturer) and laboratory processing. Material and methods: Forty human extracted maxillary premolars of approximately comparable sizes were divided into four groups: Group (A): Ten endodontically treated teeth directly filled with Filtek Z250xt without cuspal coverage. Group
... Show MoreThis work has been done with using of epoxy resin mixed with Granite powder were weighted by percent volume (5,10,15, and 20)%and then mixed with epoxy polymer to compose polymer composite. Hand lay-up technique is used in fabrication of the composite samples. Hardness test was carried out for the proper samples in both normal condition and after immersion in HCL (1 M and 2 M) solutions for periods ranging up to 10 weeks. After comparing the results between the polymer and their composite, the hardness increased with increasing Granite weight percent, it was found that Hardness were greater for the composites before immersion compared with their values after immersion.