Abstract: Tin oxide thin films were deposited by direct current (DC) reactive sputtering at gas pressures of 0.015 mbar – 0.15 mbar. The crystalline structure and surface morphology of the prepared SnO2 films were introduced by X-ray diffraction (XRD) and atomic force microscopy (AFM). These films showed preferred orientation in the (110) plane. Due to AFM micrographs, the grain size increased non-uniformly as the working gas pressure increased.
Bigheaded carps (bighead carp, Hypophthalmichthys molitrix, and silver carp, Hypophthalmichthys nobilis) and their hybrids play an important ecological and economic role in their original habitat, while their introduced stocks may pose serious ecological risks. To address questions about the persistence and invasiveness of these fish, we need to better understand their population structures. The genetic structures of bigheaded carp populations inhabiting Lake Balaton and the Tisza River were examined with ten microsatellite markers and a mitochondrial DNA marker (COI). The Lake Balaton stock showed higher genetic diversity compared with the Tisza River stock. Based on hierarchical clustering, the Tisza population was characterized o
... Show More In this research we prepared thin films from pure polymer (polyvinyl alcohol PVA )and doped with CuO with concentration 8% ,and Fe2Cl3 at different concentrations (1,5,8)%.This films were prepared by casting method and placed in Britidish (4cm diameter )with thickness(200±5)μm.Through the investigation of(X-ray )diffraction it is found all that the samples have polycrystalline structure .Also we measurement the optical properties from this films such as absorption ,transmittion spectra ,absorption coefficient ,energy gap ,extinction coefficient ,refraction index ,finesse coefficient ,the dielectric constant with two parts the real and the imaginary and the optical conductivity .
A nanocrystalline CdS thin film with 100 nm thickness has been prepared by thermal evaporation technique on glass substrate with substrate temperature of about 423 K. The films annealed under vacuum at different annealing temperature 473, 523 and 573 K. The X-ray diffraction studies show that CdS thin films have a hexagonal polycrystalline structure with preferred orientation at (002) direction. Our investigation showed the grain size of thin films increased from 9.1 to 18.9 nm with increasing the annealing temperature. The optical measurements showed that CdS thin films have direct energy band gap, which decreases with increasing the annealing temperature within the range 3.2- 2.85 eV. The absorbance edge is blue shifted. The absorption
... Show MoreIn the present work we prepared heterojunction not homogenous CdS/:In/Cu2S) by spray and displacement methods on glass substrate , CdS:In films prepared by different impurities constration. Cu2S prepared by chemical displacement method to improve the junction properties , structural and optical properties of the deposited films was achieved . The study shows that the film polycrystalline by XRD result for all film and the energy gap was direct to 2.38 eV with no effect on this value by impurities at this constration .
The structural, optical and electrical properties of ZnS films prepared by vacuum
evaporation technique on glass substrate at room temperature and treated at different
annealing temperatures (323, 373, 423)K of thickness (0.5)µm have been studied. The
structure of these films is determined by X-ray diffraction (XRD). The X-ray diffraction
studies show that the structure is polycrystalline with cubic structure, and there are strong
peaks at the direction (111).
The optical properties investigated which include the absorbance and transmittance
spectra, energy band gab, absorption coefficient, and other optical constants. The results
showed that films have direct optical transition. The optical band gab was
The structural, optical and electrical properties of ZnS films prepared by vacuum evaporation technique on glass substrate at room temperature and treated at different annealing temperatures (323, 373, 423)K of thickness (0.5)µm have been studied. The structure of these films is determined by X-ray diffraction (XRD). The X-ray diffraction studies show that the structure is polycrystalline with cubic structure, and there are strong peaks at the direction (111). The optical properties investigated which include the absorbance and transmittance spectra, energy band gab, absorption coefficient, and other optical constants. The results showed that films have direct optical transition. The optical band gab was found to be in the range t
... Show More