A single-crystalline semi-polar gallium nitride (11-22) was grown on m-plane (10-10) sapphire substrate by metal organic chemical vapor deposition. Three-step approach was introduced to investigate the grain size evolution for semi-polar (11-22) GaN. Such approach was achieved due to the optimized gallium to ammonia ratio and temperature variations, which led to high quality (11-22) oriented gallium nitride epilayers. The full width at half maximum values along (-1-123) and (1-100) planes for the overgrowth temperature of 1080°C were found to be as low as 0.37° and 0.49°, respectively. This was an indication of the enhanced coalescence and reduction in root mean square roughness as seen by atomic force microscopy. Surface analysis via atomic force microscopy indicated the orientation towards semi-polar plane. Field emission scanning electron microscopy analysis further indicates that higher temperature of 1080°C during the deposition of the overgrowth promoted closely packed surface coalescence. Room temperature Raman revealed that the overgrowth temperature of 1080°C portrayed compressive strain free as compared to other overgrowth temperature. Based on these results, the promising overgrowth temperature of 1080°C can be further utilized in future work for optoelectronics devices.
The effect of 532nm Diode Pumped Solid State (DPSS) laser at power density of 5.234 W/cm2 on the growth of Gram-negative Pseudomonas aeruginosa and Gram-positive Staphylococcus aureus was evaluated. These bacteria were isolated from samples taken from burn and infected wound areas of 55 patients admitted to the burn-wound unit in Al-Kindy teaching hospital in Baghdad during the period from October 2012 to March 2013. Each isolate was identified using microscopic, cultural and biochemical methods. A standard bacterial suspension was prepared for each isolate. Serial dilutions were then prepared and a dilution of 10-5 was selected. Irradiation experiments included four groups: (L-P-) bacterial suspension in saline solution, (L-P+) bacteria
... Show MoreA polycrystalline CdTe film has been prepared by thermal evaporation technique on glass substrate at substrate temperature 423 K with 1.0 m thicknesses. The film was heated at various annealing temperature under vacuum (Ta =473, 523 and K). Some of physical properties of prepared films such as structural and optical properties were investigated. The patterns of X-ray diffraction analysis showed that the structure of CdTe powder and all films were polycrystalline and consist of a mixture of cubic and hexagonal phases and preferred orientation at (111) direction.
The optical measurements showed that un annealed and annealed CdTe films had direct energy gap (Eg). The Eg increased with increasing Ta. The refractive index and the real p
The purpose of this paper is to study a new types of compactness in the dual bitopological spaces. We shall introduce the concepts of L-pre- compactness and L-semi-P- compactness .
The study aimed to : - To determine whether there are significant differences between Fartlek training and the increase in the molecular biology (VEGF - basal fibroblast growth factor) for arena and field players in an (800m) youth event. - Determine whether there are statistically significant differences between Fartlek training and the increase in molecular biology and some physical variables for the players (800m) in the arena and field for youth. - Determine whether the Fartlek training method is the most appropriate to achieve statistically significant differences in the research variables for the players (800m) in the arena and field for youth. The researchers used the experimental method for its suitability and the nature of the rese
... Show MoreA field experiment was conducted during winter, 2015-16 with the objective to investigate the effect of bread wheat cultivars (Abu-Ghraib3, Ibaa99, and Alfeteh) and seed priming 100, 100, 150 mg L-1 of benzyl adenine, salicylic acid, gibberellic acid (GA3), respectively, ethanolic extract of Salix Sp., water extract of Glycyrrhiza glabra and distilled water (control) on grain growth rate (GGR), effective filling period (EFP) and accelerating of physiological maturity. Randomized complete block design with three replicates was applied. GA3×Ibaa99 surpassed others in grain yield (7.432 tonne ha-1) when gave the highest grain weight (45.13 mg grain-1) and GGR (1.5 mg grain-1 day-1) with the fastest time to start and end EFP (5 and 34 days), w
... Show MoreThe temperature influence on the fluorescence lifetime, quantum yields and non-radiative rate parameter or coumarin 460 dye dissolved in methanol was investigated in the temperature range (160-300 k). A single photon counting technique was used or measuring the fluorescence decay curves. A noticeable decrease of the fluorescence lifetime with increasing the temperature was observed. The non-radiative activation energy of 10.57 K.J. mole-1 was measured by the help of Arrhenius plot.
Current research aims to find out:
- Effect of using the active learning in the achievement of third grade intermediate students in mathematics.
- Effect of using of active learning in the tendency towards the study of mathematics for students of third grade intermediate.
In order to achieve the goals of the research, the researcher formulated the following two hypotheses null:
- There is no difference statistically significant at the level of significance (0.05) between two average of degrees to achievement
Tin Oxide (SnO2) films have been deposited by spray pyrolysis technique at different substrate temperatures. The effects of substrate temperature on the structural, optical and electrical properties of SnO2 films have been investigated. The XRD result shows a polycrystalline structure for SnO2 films at substrate temperature of 673K. The thickness of the deposited film was of the order of 200 nm measured by Toulansky method. The energy gap increases from 2.58eV to 3.59 eV when substrate temperature increases from 473K to 673K .Electrical conductivity is 4.8*10-7(.cm)-1 for sample deposited at 473K while it increases to 8.7*10-3 when the film is deposited at 673K