Myelosuppression is a serious disease that is related to the malfunction of blood cells production that leads to cytopenia which is the most serious hematologic toxicity of cancer chemotherapies including cyclophosphamide, which is a strong oxazaphosphorine [a nitrogen mustard alkylating agent] that can be used alone or combined with other chemotherapeutic agents for the treatment of different malignant diseases. It induces severe bone marrow suppression by damaging hematopoietic stem cells through the generation of oxidative stress. Fisetin is a hydrophobic polyphenolic compound with a wide range of pharmacological properties such as antioxidant, anti-inflammatory, antimicrobial, osteoprotective, antidiabetic, and anti-carcinogenic activities. The present study aims to evaluate the effects of fisetin alone and pretreatment with cyclophosphamide on some selected hematological and oxidative stress parameters in the male rats model. Animals were randomly divided into 4 groups each with 7 rats. The first group received 1% dimethyl sulfoxide (negative control group). The second group received oral fisetin. The third group received a single intraperitoneal (IP) injection of cyclophosphamide (CP) and the fourth group received fisetin for 7 constitutive days than a single IP injection of CP on day 7. Results showed that both fisetin and CP significantly reduced the total white blood cells and platelet counts compared to such counts in negative control/Group I (P<0.05) when each administered alone and in combination. Furthermore, results viewed that fisetin significantly increased GSH and SOD1, and decrease MDA levels in serum compared to such levels in CP (Group III) rats (P<0.05). The study concluded that the administration of fisetin alone causes leukopenia and thrombocytopenia and this decrease augmented in combination with CP; while exhibiting a strong antioxidant effect against CP induced-oxidative stress.
Background: Failure of resin bases were a major disadvantage recorded in the constructed dentures. Reinforcements of the repair joint with nano fillers represent an attempt to enhance the strength and durability. The purpose of the research was to estimate the influence of nano fillers reinforcement with (ZrO2 and Al2O3) on impact and transverse strength of denture bases repaired with either cold or hot processing acrylic resin. Materials and methods: A hundred and forty (140) samples were processed with hot cured resin and organized in subgroups depending on the repair materials and condition (without repair (control), repair with hot cure, cold cure, hot and cold cure reinforced with either (5% Zr2O or 0.5% Al2O3). The samples in these
... Show MoreBackground: The base of the denture is largely responsible for providing the prosthesis with retention, stability, and support by being closely adapted to the oral mucosa. However; the process of bone resorption is irreversible and may lead to an inadequate fit of the prosthesis; this can be overcome by relining. Materials and methods: Acrylic based soft denture liner is prepared by preparing polymer from purified methylmethacrylate monomer with (10-2) initiator and (30%) dibutylphthalate plasticizer concentrations. Biological properties were evaluated in comparison with the control material through subcutaneous specimens' implantation in the New Zealand rabbits. Excisional biopsies were taken after (1, 3, days 1, 2, 3, 4 weeks) period. Mic
... Show MoreIn this research, Schiff bases derived from the reaction of anthrone with different heterocyclic amines have been described. The resulted Schiff base compounds were reacted with various nucleophiles in order to obtain new heterocyclic derivatives. Chemical structures of all products were confirmed by IR, 1H-, 13C-NMR spectral data and elemental analysis. All synthesized compounds were in vitro tested against a standard strain of pathogenic microorganism including Gram +ve bacteria (Staphylococcus aureus), Gram –ve bacteria (Escherichia coli), and fungi (Candida albicans).
The aim of this study is to synthesize an easy, non-toxic and eco-friendly method. Silver nanoparticles which were synthesized by leaf extract of mint were characterized by UV-Visible Spectroscopy which appears UVVisible spectrum of demonstrated a peak 448 nm corresponding to surface Plasmon resonance of silver nanoparticles, Fourier Transform Infrared Spectroscopy (FTIR); functional groups involved in the silver nanoparticles synthesis were identified, the presence of silver nanoparticles was confirmed by X-ray diffraction (XRD) and Atomic Force Microscope (AFM) analysis clearly illustrated that the shape of silver nanoparticles was spherical and the size of the silver nanoparticles has been measured as 55- 85 nm. Evaluation of its antimic
... Show MoreThe research aims to evaluate the radioactivity in elected samples of cereals and legume which are wide human consumption in Iraq using Nuclear Track Detectors (NTDs) model CN-85.
The samples were prepared scientifically according to references in this field. After 150 days of exposure, the detector were collected and chemically treated according to scientific sources (etching chemical), nuclear effects have been calculated using the optical microscope.
Radon (222Rn) concentration and uranium (238U) were calculated in unit Bq/m3 and (ppm), the results indicate that the highest concentration of radon and uranium was in yellow corn where the concentration of radon was 137.17×102 Bq/m3 and uranium concentration 2.63 (ppm). The lowest
Background: This study compared in vitro the marginal adaptation of three different, low shrink, direct posterior composites Filtekâ„¢ P60 (packable composite), Filtekâ„¢ P90 (Silorane-based composite) and Sonic fillâ„¢ (nanohybrid composite) at three different composite/enamel interface regions (occlusal, proximal and gingival regions) of a standardized Class II MO cavity after thermal changes and mechanical load cycling by scanning electron microscopy. Materials and methods:Thirty six sound human maxillary first premolars of approximately comparable sizes were divided into three main groups of (12 teeth) in each according to the type of restorative material that was used: group (A) the teeth were restored with Filtekâ„¢ P6
... Show MoreResilient polymeric materials such as silicone elastomers are currently used for maxillofacial prostheses construction but the strength of these materials and their clinical performance need to be optimized with the addition of reinforcing fillers. This study investigates the effect of zirconia nanopowder addition on tear strength, tensile strength, elongation at break, Shore A hardness, surface roughness and cytotoxicity of VST-50 maxillofacial silicone. Silicone base was mixed with different amounts (1%, 2% and 3%) of zirconia nanopowder using a vacuum mixer. Silicone without filler was used as control for comparison. Scanning Electron Microscopy and Atomic Force Microscopy were utilized to assess the efficiency of high-shear vacuum mixin
... Show More