Aim of the study: Using surface roughness and tensile bond strength tests, the objective of this investigation was to ascertain the impact of laser surface modification on the binding strength of injectable thermoplastic acrylic denture base material to acrylic-based soft-liner material. Materials and methods: Acrylic base soft liner material was bonded to injectable thermoplastic acrylic resin (Deflex). Forty specimens were created (20 disc, 20 dumbbells) 10 of each specimen type as control specimens, and 10 were treated with nano pulse Nd: YAG laser. The data were analyzed using the Kruskal-Wallis test and unpaired t-test (a=.05) and the roughness test was performed utilizing a double column universal test machine. Results: Compared to the control groups, the laser group had much increased roughness and tensile bond strength. Conclusions. Following Nd:YAG laser surface treatment, the tensile bonding strength between acrylic soft-liner material and thermoplastic acrylic was increased.
Background: Polyetheretherketone (PEEK) is a promising implant material due to its superior biomechanical strength. However, due to its hydrophobic nature and lack of cellular adhesion properties, it has poor integration with bone tissue. Methods: A fractional CO2 laser was used with various parameters for surface texturing of PEEK substrate to enhance its surface properties. An optical microscope and field-emission scanning electron microscope (FESEM) were used to examine the surface morphology of untextured and laser-textured samples. Energy dispersive X-ray spectroscopy (EDX) was performed to determine the effect of the laser on the microstructure of PEEK. Surface microroughness, atomic force microscopy (AFM), and wettability were invest
... Show MoreThe purpose of this work was to study the effects of the Nd:YAG laser on exposed dentinal
tubules of human extracted teeth using a scanning electron microscope (SEM). Eighty 2.5mm-thick
slices were cut at the cementoenamel junction from 20 extracted human teeth with an electric saw. A
diamond bur was used to remove the cementum layer to expose the dentinal tubules. Each slice was
sectioned into four equal quadrants and the specimens were randomly divided into four groups (A to D ).
Groups B to D were lased for 2 mins using an Nd:YAG laser at 6 pulses per second at energy outputs of
80 , 100 and 120 mJ. Group A served as control. Under SEM observation, nonlased specimens showed
numerous exposed dentinal tubules. SEM o
S a mples of compact magnesia and alumina were evaporated
using CO2-laser .The
Processed powders were characterized by electron microscopy
and both scanning and transmission electron microscope. The results
indicated that the particle size for both powders have reduced largely
to 0.003 nm and 0.07 nm for MgO and Al2O3, with increasing in
shape sphericity.
An analytical method and a two-dimensional finite element model for treating the problem of laser heating and melting has been applied to aluminum 2519T87and stainless steel 304. The time needed to melt and vaporize and the effects of laser power density on the melt depth for two metals are also obtained. In addition, the depth profile and time evolution of the temperature before melting and after melting are given, in which a discontinuity in the temperature gradient is obviously observed due to the latent heat of fusion and the increment in thermal conductivity in solid phase. The analytical results that induced by laser irradiation is in good agreement with numerical results.
The purpose of this study is to investigate the biostimulation effect of 532 nm CW laser on the metabolism of Saccharomyces cerevisiae yeast. Cells were irradiated by 532 nm Nd:YAG laser using 0.153 W/cm2 power density at 30, 45, 60,180 and 300 seconds exposure times in their respective orders. Intrafluorescence parameters were measured by detection the autofluorescence intensity, proliferation rate and Imaging the fluorescent mitochondria using confocal laser scanning microscope. The results showed that the 30 and 45 second exposure times seem to have stimulated changes in the cells that led to increase proliferation, viability and mitochondrial activity. Autofluorescence of cells increased after 45 and 60 seconds exposure time. After 3
... Show MoreAbstract: The use of indirect, all-ceramic restorations has grown in popularity among dentists. Studies have demonstrated that for indirect ceramic restorations to be effective over time, cement and ceramic must be bonded in a stable manner. Chemical, mechanical, and laser irradiation are among the methods used to precondition ceramic surfaces in order to increase bond strength.The objective of the study: This study was performed to investigate the roughness values and surface topography of lithium disilicate glass-ceramic treated with conventional methods and different Er,Cr:YSGG, and fractional CO2 laser conditioning parameters.Material and methods:<
... Show MoreBackground: The aim of this study was to comparatively evaluate the push out bond strength (PBS) of root canal fillings using four different obturation techniques (single cone (SC), cold lateral compaction (CLC), continuous wave (CW), and carrier based gutta percha (CBG)). Materials and Methods: Forty mandibular premolar decoronated and instrumented with rotary ProTaper to F3 then teeth were divided randomly into 4 groups of 10 teeth for each as follow: group (I) single- cone obturation with matched-taper gutta-percha, group (II) cold lateral compaction technique, group (III) continuous wave of obturation technique, and group( IV) carrier based gutta-percha technique. Zinc oxide eugenol (ZOE) sealer was used as a root canal sealer for the
... Show More