Warm Mix Asphalt (WMA) is a modern energy-saving process that uses environmentally friendly materials, has lower mixing and compaction temperatures, and uses less energy and releases less contaminants than conventional hot mix asphalt. Moisture damage poses one of the main challenges of the material design in asphalt pavements. During its design life, the asphalt pavement is exposed to the effect of moisture from the surrounding environment. This research intends to investigate the role of the polypropylene fibres for modifying the moisture susceptibility for the WMA by using different percentages of polypropylene (namely 2, 4, and 6%) by weight of the binder of the control mixture (WMA). In this paper, the physical characteristics of the asphalt cement, Marshall properties, Tensile Strength Ratio (TSR) and Index of Retained Strength (IRS) were determined to establish the effect of the polypropylene on the moisture susceptibility of the WMA. The results displayed that the modification of the AC with polypropylene caused an increase in the optimum asphalt content by 1.03, 3.09, and 11.3%, with the addition of 2, 4 and 6% of the P.P., respectively. The moisture resistance of the asphalt mixture was enhanced by adding the P.P., according to the rise in the Tensile Strength Ratio (TSR) and Index of Retained Strength (IRS) values. The TSR value showed 9.4, 18.2 and 19.5% increase when the P.P. increased from 0.00 to 0.02, 0.04, and 0.06, respectively; besides, the IRS showed improvement with the addition of the P.P. to the WMA. Doi: 10.28991/cej-2021-03091704 Full Text: PDF
يشهد العالم تقدما في كافة مجالات الحياة المختلفة وتزداد الحياة صعوبة يوما بعد يوم, ويزداد البحث في كافة المجالات التي تعمل على خدمة الإنسان ولقد طال هذا التقدم النشاط الرياضي ,فقد يكون لتطور التدريب الرياضي وتنوع أساليبه الدور الكبير في تحقيق اللياقة البدنية التي تعد إحدى أهم الأهداف التي يرمي إليها الدرس في كلية التربية الرياضية . واللياقة البدنية تستمد أهميتها من كونها إحدى مكونات اللياقة الشاملة التي بدو
... Show MoreThe performance and lifetime of the flexible asphalt pavement are mainly dependent on the interfacial bond strength between layer courses. To enhance the bond between layers, adhesive materials, such as tack coats, are used. The tack coat itself is a bituminous material, which is applied on an existing relatively non-absorbent surface to ensure a strong bond between the old and newly paved layer. The primary objective of this study was to evaluate the effects of various types of tack coat materials on interlayer bond strength and to determine the optimal application rate for each type. The tack coat types used in this paper were RC-70, RC-250, and CSS-1h. Both laboratory-prepared and field-constructed hot mix asphalt concrete pavements usin
... Show MorePseudomonas aeruginosa gram-negative, bacilli and facultative aerobic, P. aeruginosa cause cystic fibrosis patients, wounds, burns, and immunodeficienct patients, that have many virulence factors such as pyocyanin , cytotoxic ,biofilm formation and motility, Eighty-eight isolates belonging to P. aeruginosa were collected including the 66 clinical isolates obtained from different hospitals in Baghdad and were from different sources and 22 environmental isolates from previous studies of soil near oil fields. Microscopical and cultural characteristics were studied and diagnosed using biochemical tests, VITEC device, their ability to adhere to non-living (Polystyrene), living cell line (A549) and cytotoxicity of bacterial filtrate
... Show MoreRutting has a significant impact on the pavements' performance. Rutting depth is often used as a parameter to assess the quality of pavements. The Asphalt Institute (AI) design method prescribes a maximum allowable rutting depth of 13mm, whereas the AASHTO design method stipulates a critical serviceability index of 2.5 which is equivalent to an average rutting depth of 15mm. In this research, static and repeated compression tests were performed to evaluate the permanent strain based on (1) the relationship between mix properties (asphalt content and type), and (2) testing temperature. The results indicated that the accumulated plastic strain was higher during the repeated load test than that during the static load tests. Notably, temperatur
... Show MoreThis research delves into the realm of asphalt technology, exploring the potential of nano-additives to enhance traditional asphalt binder properties. Focusing on Nano-Titanium Dioxide (NT), Nano-Aluminum Oxide (NA), and Nano-Silica Oxide (NS), this study investigates the effects of incorporating these nanomaterials at varying dosages, ranging from 0% to 8%, on the asphalt binder’s performance. This study employs a series of experimental tests, including consistency, storage stability, rotational viscosity, mass loss due to aging, and rheological properties, to assess the impact of nano-additives on asphalt binder characteristics. The findings indicate a substantial improvement in the consistency of the asphalt binder with the add
... Show MoreThis research delves into the realm of asphalt technology, exploring the potential of nano-additives to enhance traditional asphalt binder properties. Focusing on Nano-Titanium Dioxide (NT), Nano-Aluminum Oxide (NA), and Nano-Silica Oxide (NS), this study investigates the effects of incorporating these nanomaterials at varying dosages, ranging from 0% to 8%, on the asphalt binder’s performance. This study employs a series of experimental tests, including consistency, storage stability, rotational viscosity, mass loss due to aging, and rheological properties, to assess the impact of nano-additives on asphalt binder characteristics. The findings indicate a substantial improvement in the consistency of the asphalt binder with the add
... Show MoreIn this study, silver nanoparticles (AgNPs) were synthesized using a cold plasma technique and a plasma jet. They were then used to explore how photothermal treatment may be used to treat lung cancer (A549) and normal cells (REF) <i>in vitro</i>. The anti-proliferative activity of these nanoparticles was studied after A549 cells were treated with (AgNPs) at various concentrations (100%, 50%, or 25%) and exposure times (6 or 8 min) of laser after 1 h or 24 h from exposed AgNPs. The highest growth inhibition for cancer cells is (75%) at (AgNPs) concentration (100%) and the period of exposure to the laser is (8 min). Particle size for the prepared samples varied according to the diameter o
... Show MoreActivity test of the inhibitors purified from barley and broad beans crop proved the inhibition activity against 6 types of rots Pencillium ssp and Aspergellusflavus and Aspergillus niger and Fusarium solani and Fusarium semitectum and Mucor with three concentrations 0.1 and 0.2 and 0.3 mg/ml, where the inhibitor purified from the second peak of broad beans proved that it had a higher inhibition activity against the growth of test rots which were 53.75 and 62.5 and 78.5 and 76.25 and 84 and 18.8% respectively, at 0.3 mg/ ml followed by the first peak of the inhibitor purified from broad beans the inhibition activity were 43.75 and 50 and 62.96 and 75 and 80 and 12.5 then the inhibitor purified from barley in which the inhibition activity
... Show MoreBackground: Sperm motility disorder is an important cause of infertility in male, and one of the causes of reduced motility of the sperm is the disorders of the mitochondria because it provides the required energy for sperm motility, Laser biostimulation or low-level laser therapy has a positive effect on the mitochondria and led to increasing the synthesis of ATP. Method: Twenty fresh human semen samples were used in this research study, each sample was separated into two portions, one was used as control which is not exposed to the laser beam and the other was irradiated with the wavelength of 410 nm diode laser with an output power of 100 mW and an exposure time of 60 seconds, then the measurement of
... Show More