Our research aimed to find a new material that can be an efficient heavy metal free flame retardant for plasticized poly(vinyl chloride) comparable to the conventional flame retardants. One of these extraordinary materials is Oxydtron using as an admixture for concrete. Oxydtron showed unexpected efficiency as a flame retardant agent and an excellent heat stabilizer as well. Limiting oxygen index (LOI), static heat stability, Congo-red, and differential scanning calorimetry (DSC) were carried out. The thermal tests proved that Oxydtron is suitable to improve plasticized poly(vinyl chloride) performance at high temperatures applications in terms of flame retarding and thermal stability. Therefore, the positive result obtained by the addition of Oxydtron is reducing of plasticized poly(vinyl chloride) flammability by 25.23%, and increasing its thermal stability as well.
Ultrasonic absorption, velocity, viscosity, adiabatic compressibility, relaxation time and relaxation amplitude measurements are reported on different concentrations of poly(acrylic acid) solutions in common solvent water using pulsed ultrasonic apparatus technique operating at 26 kHz and 30 ºC. Results show an increase of velocity, viscosity, and absorption coefficient ،relaxation time and relaxation amplitude values with the increasing concentrations of the poly(acrylic acid) solutions, which might be the result of structural fluctuations of polymer molecules such as the segmental motions of the polymer chains. In contrast the compressibility decreases with the increasing concentration of this polymer. This study suggests there i
... Show MoreThe influence and hazard of fire flame are one of the most important parameters that affecting the durability and strength of structural members. This research studied the influence of fire flame on the behavior of reinforced concrete beams affected by repeated load. Nine self- compacted reinforced concrete beams were castellated, all have the same geometric layout (0.15x0.15x1.00) m, reinforcement details and compressive strength (50 Mpa).
To estimate the effect of fire flame disaster, four temperatures were adopted (200, 300, 400 and 500) oC and two method of cooling were used (graduated and sudden). In the first cooling method, graduated, the tested beams were leaved to cool in air while in the seco
... Show MoreThe influence and hazard of fire flame are one of the most important parameters that affecting the durability and strength of structural members. This research studied the influence of fire flame on the behavior of reinforced concrete beams affected by repeated load. Nine self- compacted reinforced concrete beams were castellated, all have the same geometric layout (0.15x0.15x1.00) m, reinforcement details and compressive strength (50 Mpa). To estimate the effect of fire flame disaster, four temperatures were adopted (200, 300, 400 and 500) oC and two method of cooling were used (graduated and sudden). In the first cooling method, graduated, the tested beams were leaved to cool in air while in the second method, sudden, water splash was use
... Show MoreAn experimental program was conducted to determine the residual of composite Steel Beams-Reinforced Concrete (SB-RC) deck floors fabricated from a rolled steel beam topped with a reinforced concrete slab, exposed to high temperatures (fire flame) of 300, 500, and 700ºC for 1 hour, and then allowed to cool down by leaving them in the lab condition to return to the ambient temperature. The burning results showed that, by exposing them to a fire flame of up to 300ºC, no serious permanent deflection occurred. It was also noticed that the specimen recovered 93% of 19.2 mm of the deflection caused by burning. The recovered deflection of burned composite SB-RC deck floor at 500ºC was 40% of 77.9 mm of the deflection caused by burning with a res
... Show MoreA new method for the determination of the drug cefalexin in some Pharmaceuticals using (UV-Vis) and indirect Flame Atomic Absorption Spectrophotometer (FAAS) , Fe III should forms a chelating complex with cefalexin (CEX –Fe III) at pH (1-8) and the best pH for the formation of (CEX –Fe III) chelating complex was (2) .The complex extracted with Methanol and Dimethy-Sulphoxide .The mole-ratio method has been used to determine the structure of chelate (CEX - Fe III) and found to be 2:1 LM ( Ligand : Metal.) .
Keywords : Cefalexin , chelating complex.
Metronidazole-MIPs were prepared by using (MDZ) as the template as well as allylchloride (AYC) or allylbromide (AYB) as monomer, used (TMPTA) tri-methylol propane tri-acrylate or ethylene glycol di-methyl acrylate (EGDMA) as cross-linker and initiator used (BP) benzyl peroxide. By using different plasticizers (di butyl Phthalate (DBPH), Nitrobenzene (NB), oleic acid (OA) and paraffin) for MDZ-MIP1 and (Di-butyl sebecate (DBS), Di-methyl acrylate (DMA), Tributylphosphate(TBP) and Tris(ethylhexyl phosphate (TEHP) ) for MDZ-MIP2. Membranes of MIPs were prepared in PVC matrix. The characterizations of each electrode were determined The Slope range from (55.083 - 43.711) mV/decade, Limit of Detection (8 X 10 -4- 2 X 10-6) and Linearity
... Show MoreThe heavy metal cadmium is extremely harmful to both humans and animals. Zinc supplementation protects the biological system and reduces cadmium-induced toxicity. This study aimed to determine whether zinc chloride (ZnCl2) could protect male mice with the damaged liver induced by cadmium chloride (CdCl2). The protective role of zinc chloride and expression of the metallothionein (MT), Ki-67, and Bcl-2 apoptotic proteins in hepatocytes were studied after subchronic exposure of mice to cadmium chloride for 21 days. Thirty male mice were randomly categorized into 6 groups (5 mice/group) as follows: a control group that did not receive any treatment, a group given ZnCl2 at 10 mg/kg alone, and two groups received ZnCl2 (10 mg/kg) i
... Show More