This study includes the manufacture of four ternary alloys represented S60Se40-XPbX with weight ratios x = 0, 10, 20, and 30 by the melting point method. The components of each alloy were mixed separately, then placed in quartz ampoules and vacuumed out with a vacuum of roger that 10−4 Torr. The ampule was heated in two stages to avoid sudden dissipation and precipitation of selenium on the inner mass of the quartz tube. The ampoule was gradually heated and kept at 450°C for approximately 4 hours followed by 950°C for 10 hours.at a rate of 10 degrees Celsius, the temperature of the electric furnace was increased, and then the ampoule was subjected to rapid cooling with cold water to reach a state of solidity glass-like. The research aims to investigate the effect of adding lead to selenium on the properties of thermal conductivity and heat flux density. It has been noted that the partial replacement of selenium with lead affected these properties significantly.
six specimens of the Hg0.5Pb0.5Ba2Ca2Cu3-y
This research is devoted to the effect of investigation of the ZnO content on the structural and electrical properties of (NiO)1-x (ZnO)x films prepared by pulsed laser precipitation on the glass substrate at room temperature. Thin-film (NiO)1-x (ZnO)x sediments were deposited with different composition ratios where x = 0, 0.2, 0.4, 0.6 and 1.0 with a thickness of n150nm. The diffraction pattern for X-ray analysis reveals that the structure of the prepared thin films is identical with the cubic phase and hexadecimal stage of x = 0 and 0.1, respectively while the structure is mixed with the remaining x
Zinc-indium-selenide ZnIn2Se4 (ZIS) ternary chalcopyrite thin film on glass with a 500 nm thickness was fabricated by using the thermal evaporation system with a pressure of approximately 2.5×10−5 mbar and a deposition rate of 12 Å/s. The effect of aluminum (Al) doping with 0.02 and 0.04 ratios on the structural and optical properties of film was examined. The utilization of X-ray diffraction (XRD) was employed to showcase the influence of aluminum doping on structural properties. XRD shows that thin ZIS-pure, Al-doped films at RT are polycrystalline with tetragonal structure and preferred (112) orientation. Where the
Bulk AlxSb1-x samples were prepared with different x ratios (0.1, 0.3, 0.5, 0.7 and 0.9) by quenching technique. This was done throughout mixing the aluminum and antimony elements according to the proper atomic weight and put them in an evacuated quartz ampoule which then sealed and heated at 1273 K for five hours and left to cool in air. Thin films of AlxSb1-xwere prepared by using thermal evaporation under vacuum of 10-5 mbar on glass substrates at room temperature with deposition rate (10-15nm/min) at thickness of ∼ 500nm. The structures of AlxSb1-x bulk and thin films have been studied by X–ray diffraction technique. The results showed that all alloys have polycrystalline structures and the p
The non-linear components has been emphasized for its multiple applications in rewritable recording and data storage devices. Chalcogenide glasses materials are promising due to their high refractive index. In this paper, alloys for Ge30Te70-xSbxglasses semiconductor (where x =0.0, 5, 10, 15 and 20) will be fabricated by melt quenching method. The effect of partial substitution on DC electric power parameters, and its knowledge of electrical conduction mechanisms, were investigated to determine the effect of Antimony on the density of extended states, local states, and in Fermi energy states. The electrical measurements revealed the existence of three conduction mechanis
... Show MoreIn this manuscript, the effect of substituting strontium with barium on the structural properties of Tl0.8Ni0.2Sr2-xBrxCa2Cu3O9-δcompound with x= 0, 0.2, 0.4, have been studied. Samples were prepared using solid state reaction technique, suitable oxides alternatives of Pb2O3, CaO, BaO and CuO with 99.99% purity as raw materials and then mixed. They were prepared in the form of discs with a diameter of 1.5 cm and a thickness of (0.2-0.3) cm under pressures 7 tons / cm2, and the samples were sintered at a constant temperature o
... Show MoreThis work concerned with effect of zinc oxide concentrating on the structural and optical properties of (MgO)1-x(ZnO)x thin films. (MgO)1-x(ZnO)x compounds were produced by mixing the two oxides powders accordance to the atomic ratios and compressed as pellets, these pellets were sintered in an oven at temperature1273K for five hours. Thin films from (MgO)1-x(ZnO)x compounds were obtained using pulsed laser deposition technique using Nd:YAG laser . The results of x-ray diffraction as well as UV-Visible- spectrophotometer measurements transmittance of (MgO)
Thin films of (CuO)x(ZnO)1-x composite were prepared by pulsed laser deposition technique and x ratio of 0≤ x ≤ 0.8 on clean corning glass substrate at room temperatures (RT) and annealed at 373 and 473K. The X-ray diffraction (XRD) analysis indicated that all prepared films have polycrystalline nature and the phase change from ZnO hexagonal wurtzite to CuO monoclinic structure with increasing x ratio. The deposited films were optically characterized by UV-VIS spectroscopy. The optical measurements showed that (CuO)x(ZnO)1-x films have direct energy gap. The energy band gaps of prepared thin films
The compound Fe0.5CoxMg0.95-xO where (x= 0.025, 0.05, 0.075, 0.1) was prepared via the sol-gel technique. The crystalline nature of magnesium oxide was studied by X-ray powder diffraction (XRD) analysis, and the size of the sample crystals, ranging between (16.91-19.62nm), increased, while the lattice constant within the band (0.5337-0.4738 nm) decreased with increasing the cobalt concentration. The morphology of the specimens was studied by scanning electron microscopy (SEM) which shows images forming spherical granules in addition to the presence of interconnected chips. The presence of the elements involved in the super