Abstract: Under high-excitation irradiance conditions to induce fluorescence, the dependence of photobleaching of Coumarin 307 (C307) and acriflavine (ACF) laser dyes in liquid and solid phases have been studied. A cw LD laser source of 1 mW and 407 nm wavelength was used as an exciting source. For one hour exposure time, it was found that the solid dye samples suffer photobleaching more than the liquid dye samples. This is because in liquid solutions the dye molecules can circulate during the irradiation, while the photobleaching is a serious problem when the dye is incorporated into solid matrix and cannot circulate.
A series of new coumarin and N-amino-2-quinolone derivatives have been synthesized. The reaction of coumarin (1) with excess of Hydrazine hydrate 98% yielded 1-amino-2-quinolone (2), Compound (2) was reacted with different Sulfonyl chloride to yield Sulfonamides [ N-(2-oxoquinolin-1(2H)-yl) methane sulfonamide (3), N-(2-oxoquinolin-1(2H)-yl) Benzene sulfonamide (4) and 4-methyl-N-(2-oxoquinolin-1(2H)-yl) benzene sulfonamide (5) ], while reaction of 2-(4-methyl-2-oxo-2H-chromen-7-yloxy) acetic acid (8) with different amines yielded compounds [ 2-(4-methyl-2-oxo-2H-chromen-7-yloxy)-N-(2-oxoquinolin-1(2H)-yl) acetamide (9) and N-(5-methyl-1,3,4-thiadiazol-2-yl)-2-(4-methyl-2-oxo-2H-chromen-7-yloxy)acetamide (10) ] th
... Show MoreThe relation between the output power and wavelengths for a 532nm 3W frequency doubled diode pumped solid state laser pumped Ti:Sapphire crystal is investigated. A 20 femtosecond pulse at 800 nm is obtained. A 320 mW is found to be the highest power at 800nm. Below this wavelength value and above the power was found to deviate from highest output value.
Abstract: When it comes to applications in welding, cutting, and surface engineering, the utilization of high-power fiber-delivered beams from solid-state lasers offers several benefits. This paper addresses the issue of cleaning the surface of the samples with different spot sizes (50, 100 and 200) (industrial ytterbium fiber laser) to prepared it to be welded. Angular laser cleaning with incident angles (5, 10, 15, 20, 25, 30) ° with different powers (3, 5, 7, 10) W and hatch distance 0.001 was use for implemented.
In this study three reactive dyes (blue B, red R and yellow Y) in single , binary and ternary solution were adsorbed by activated carbon AC in equilibrium and kinetic experiments. Surface area, Bulk and real density, and porosity were carried out for the activated carbon.
Batch Experiments of pH (2.5-8.5) and initial concentration (5-100) mg/l were carried out for single solution for each dye. Experiments of adsorbent dosage effect (0.1-1)g per 100 ml were studied as a variable to evaluate uptake% and adsorption capacity for single dyes(5, 10) ppm, binary and ternary (10) ppm of mixture solutions solution of dyes. Langmuir, and Freundlich, models were used as Equilibrium isotherm models for single solution. Extended Langmuir and Freun
Nano TiO2 thin films on glass substrates were prepared at a constant temperature of (373 K) and base vacuum (10-3 mbar), by pulsed laser deposition (PLD) using Nd:YAG laser at 1064 nm wavelength. The effects of different laser energies between (700-1000)mJ on the properties of TiO2 films was investigated. TiO2 thin films were characterized by X-ray diffraction (XRD) measurements have shown that the polycrystalline TiO2 prepared at laser energy 1000 mJ. Preparation also includes optical transmittance and absorption measurements as well as measuring the uniformity of the surface of these films. Optimum parameters have been identified for the growth of high-quality TiO2 films
... Show MoreSawdust has the ability to adsorb the dyestuff from aqueous solution. It may be useful low cost adsorbent for the treatment of effluents, discharged from textile industries. The effectiveness of sawdust has been tested for the removal of color from the wastewater samples containing two dyes namely Direct Blue (DB) and Vat Yellow (VY). Effect of various parameters such as agitation time, adsorbent dose and initial concentration of each dye has been investigated in the present study. The adsorption of dyes has been tested with various adsorption isotherm models. The Langmuir isotherms model is found to be the most suitable one for the dye adsorption using sawdust and the maximum adsorption capacity is 8.706 mg/g and 6.975 mg/g for DB and V
... Show MoreAbstract: Objectives: To investigate the effect of temperature elevation on the bonding strength of resin cement to the zirconia ceramic using fractional CO2 laser. Background: Fractional CO2 laser is an effective surface treatment of zirconia ceramic, as it increases the bonding strength of zirconia to resin cement. Methods: Thirty sintered zirconia discs (10 mm diameter, 2 mm thickness) were prepared and divided to three groups (N=10) and five diffident pulse durations were used in each group (0.1, 0.5, 1, 5 and 10 ms). Group A was treated with 10 W power setting, group B with 20 W and group C with 30 W. During laser irradiation, temperature elevation measurement was recorded for each specimen. Luting cement was bonded to the treated z
... Show MoreIn the present work, different thicknesses of CdS film were prepared by chemical bath deposition. Z-Scan technique was used to study the nonlinear refractive index and nonlinear absorption coefficients. Linear optical testing were done such as transmission test, and thickness of films were done by the interference fringes (Michelson interferometer). Z-scan experiment was performed at 650nm using CW diode laser and at 532nm wavelength. The results show the effect of self-focusing and defocusing that corresponds with nonlinear refraction n2. The effect of two-photon absorption was also studied, which correspond to the nonlinear absorption coefficient B.
This research aims to find how three different types of mouthwashes affect the depth of artificial white spot lesions. Teeth with various depths of white spot lesions were immersed in either splat mouthwash, Biorepair mouthwash, Sensodyne mouthwash, or artificial saliva (control)twice daily for one minute for 4 weeks and 8 weeks at 37°C. After this immersion procedure, lesion depth was measured using a diagnosed pen score. A one-way analysis of variance, Dunnett T3 and Tukey's post hoc α = .05 were used to analyze the testing data. Splat mouthwash enhanced the WSL remineralization and made the lowest ΔF compared with other mouthwashes in shallow and deep enamel after 4 and 8 weeks of treatment. In the repair groups, after 4 weeks