A series of coumarin derivatives linked to amino acid ester side chains were synthesized and evaluated of their antibacterial and antifungal activity. The coumarin derivatives was alkylated by the ethyl bromoacetate and then using potassium carbonate to get alkylated hymecromone. Conventional solution method for amide bond formation was used as a coupling method between the carboxy-protected amino acids with acetic acid side chain of coumarin derivatives. The DCC/ HOBt coupling reagents were used for peptide bond formation. The proposed analogues were successfully synthesized and their structural formulas were consistent with the proposed struct
... Show MoreIn this study, the construction of axial load-bending moment interaction diagrams for a reinforced concrete column and a steel jacket column has been presented. For a reinforced concrete column strengthened with a steel jacket consist of vertical steel sections connected by horizontal steel plates (battens), the axial load-bending moment interaction diagrams have been constructed using two analytical methods: strain compatibility method and plastic stress distribution method. In the strain compatibility method, the effects of position of the neutral axis on the stress of concrete, reinforcing bars, and steel section have been taken into consideration. In the plastic stress distribution method, the position of the neutral axis has no effect
... Show MoreThe corrosion inhibition of aluminum alloy 5083 by an environment friendly compound called (8- Hydroxyquinoline) in
acidic and alkaline solutions of pH (2 and 12) respectively were studied using weight loss and polarization techniques.
Also to examine the main and combined effects of the inhibitor concentration, pH, and contact time using factorial
experimental design. Results show that corrosion rate decreased with increasing both inhibitor concentration and
contact time and increased with increasing pH value. The polarization curves show that 8-hydroxyquinoline is a
cathodic inhibitor
This work investigates the utilization of waste papers (natural and industrial) i.e (citrus aurantium and papers A4) mortars containing specified contents 0.5%, 1%, 1.5% of waste papers were prepared and cured. Mechanical characteristics such as compressive and bending strengths, hardness and water absorption were determined for the mortars mixed with the waste papers and compared with those obtained from the pure mortars. Results showed that the addition of waste paper leads to increase the hardness to (69 - 68.5) shore D for (natural and industrial) wastes materials respectively comparing with pure specimen 66 shore D. The compressed strength of the mortar cement specimen cured for 28 days from 13 MPa to (17-18) MPa for (natural and in
... Show MoreAbstract: This study aims to investigate the effects of solvents of various polarities on the electronic absorption and fluorescence spectra of RhB and Rh6G. The singlet‐state excited dipole moments (me) and ground state dipole moments (mg) were estimated from the equations of Bakshiev -Kawski and Chamma‐ Viallet using the variation of Stokes shift along with the solvent’s dielectric constant (e) and refractive indexes (n). The observed singlet‐state excited dipole moments were found to be larger than the ground‐state ones. Moreover, the obtained fluorescence quantum yield values were influenced by the environment of the fluorescing molecule. Consequently, the concentration of the dye solution, excited singlet state absorption and
... Show MoreThis research explored the performance of steel fiber concrete-filled stainless-steel tube columns stiffened with embedded carbon steel T-sections with various steel fiber ratios under biaxial bending conditions. A numerical parametric analysis was adopted, using finite element modeling with Abaqus CAE/2021 to evaluate the effects of the fiber ratio (ranging from 0% to 1.5%) on the load-bearing capacity and deflection behavior of columns. In addition, the compressive strength of concrete ranged between 45 and 65 MPa. An increase in the fiber ratio led to a substantial improvement in the ultimate load-bearing capacity (up to 24%), a reduction in deflection (of approximately 49%), and an improvement in column ductility, which were obt
... Show More