The present study utilised date palm fibre (DPF) waste residues to adsorb Congo red (CR) dye from aqueous solutions. The features of the adsorbent, such as its surface shape, pore size, and chemical properties, were assessed with X-ray diffraction (XRD), BET, Fourier-transform infrared (FTIR), X-ray fluorescence (XRF), and field emission scanning electron microscope (FESEM). The current study employed the batch system to investigate the ideal pH to adsorb the CR dye and found that acidic pH decolourised the dye best. Extending the dye-DPF waste mixing period at 25°C reportedly removed more dye. Consequently, the influence of the starting dye and DPF waste quantity on dye removal was explored in this study. At 5 g/L dye concentration, 48% dye removal was achieved, whereas at low dye concentrations, only 40% of the dye was removed. The current study also evaluated the DPF particle size created for dye adsorption, yielding a 66% optimal powder size removal. The heat impact assessment performed in this study indicated that increased temperature affected the amount of dye eliminated from aqueous solutions, where a 72% removal was recorded at 45°C. The pseudo-first- and pseudo-second-order models were utilised to predict the maximum CR dye adsorption with DPF waste. Resultantly, the Langmuir-Freundlich experimental DPF waste CR adsorption documented pseudo-second-order kinetics. In a fixed bed reactor, the DPF waste has been reported to remove CR dye constantly. Consequently, several factors affecting the removal process, including the effects of primary dye, the flow rate of the liquid inside the column, the depth of the filling inside the column, and flow rate were assessed. The results were simulated in the COMSOL® program and compared to practical experiments, which yielded a 99% match. Conclusively, DPF waste could remove several colours from wastewater via active removal.
A simple indirect spectrophotometric method for determination of mebendazol in pure and pharmaceutical formulation was presented in this study. UV-Visible spectrophotometry using the optimal conditions was developed for determination of mebendazole in pure drug and different preparation samples. The method is based on the oxidation of drug by nbromosuccinimide with hydrochloric acid and the left amount of oxidizing agent was determined by the reaction with tartarazine and the absorbance was measured at 428 nm. Calibration curves were linear in the range of 5 to 30 µg.mL-1 with molar absorptivity 8437.2 L.mol-1 .cm-1 . The limits of detection and quantification were determined and found to be 0.7770 µg.mL-1 and 2.3400 µg.mL-1 respec
... Show MoreThis study was concerned with the adsorption of Toluene ,0·
nitro Toluene and 2,4.dinitro Toluene on The surface of kaolin clay.
The adsorption isotherms were of types( S3,S4 ) according to Giles classification and were in a good correlation with Freundlich equation in the range of cuncenlraliuns studied. The re5ult indicated that adsorption capacity increase with the increase of equilibrium concentration. The effect of the nwnber of substituted nitro groups in the adsorption extent of toluene was found to decrease in the following order:·
Toluene > 2,4-dinitro toluene > 0-nitro toluene
Adsorption on kaolin surface were examined as afunction
... Show MoreThe coefficient of charge transfer at heterogeneous devices of Au metal with a well-known dyeis investigations using quantum model.Four different solvent are used to estimation the effective transition energy. The potential barrier at interface of Au and dye has been determined using effective transition energy and difference between the Fermi energy of Au metal and ionization energy of dye. A possible transfer mechanism cross the potential barrier dyeand coupling strength interaction between the electronic levels in systems of Au and is discussed.Differentdata of effective transition energy and potential barrier calculations suggest that solvent is more suitable to binds Au with dye.
This work describes the enhancement of phenol red decolorization through immobilizing of laccase in chitosan and enzyme recycling. Commercial laccase from white rot fungus, Trametesversicolor (Tvlac), was immobilizedin to freshly prepared chitosan beads by using glutaraldehyde as a cross linker. Characterization of prepared chitosan was confirmed by FTIR and scanning electron microscope (SEM). Tvlac (46.2 U/mL) immobilized into chitosan beads at 0.8 % glutaraldehyde (v/v) within 24 hrs. Synthetic (HBT) and natural (vanillin) mediators were used to enhance dye decolorizoation. It was found that 89 % of phenol red was decolorized by chitosan beads within 180 min. in the absence of enzyme and mediator, while decolorization percenta
... Show MoreIn this work, enhancement to the fluorescence characteristics of laser dye solutions hosting highly-pure titanium dioxide nanoparticles as random gain media. This was achieved by coating two opposite sides of the cells containing these media with nanostructured thin films of highly-pure titanium dioxide. Two laser dyes; Rhodamine B and Coumarin 102, were used to prepare solutions in hexanol and methanol, respectively, as hosts for the nanoparticles. The nanoparticles and thin films were prepared by dc reactive magnetron sputtering technique. The enhancement was observed by the narrowing of fluorescence linewidth as well as by increasing the fluorescence intensity. These parameters were compared to those of the dye only and the dye solution
... Show MoreThe aims of this study are to measure the defect rate and analyze the problems of production of ready concrete mixture plant by using Six Sigma methodology which is a business strategy for operations improvement depending basically on the application of its sub-methodology DMAIC improvement cycle and the basic statistical tools where the process sigma level of concrete production in the case study was 2.41 σ.