Steel Reinforced Concrete (RC) frequently faces durability problems. In certain areas, Glass Fiber-Reinforced Polymer (GFRP) rebars are considered a non-corrodible substitute for steel reinforcement. Elevated temperatures have a significant impact on the mechanical characteristics and the adhesiveness of GFRP rebars to concrete, particularly when the polymeric matrix's glass transition temperature is approached or surpassed. Three simply supported reinforced concrete slabs were considered in the experimental program. Each specimen had identical dimensions of 1500×540×120 mm. For the fire resistance requirements, a 45 mm clear concrete cover and an exception of a 200 mm unexposed (cool) anchor zone at the ends were considered. The GFRP replacement ratio was 0, 20, and 40%. The burning procedure involved fire exposure for an hour with a steady-state temperature of 500 °C in accordance with ASTM E-119 regarding the temperature time elevation and a sudden cooling condition. The optimal concrete cover was detected by testing a fire-exposed small model reinforced by GFRP bars of varying concrete cover. The specimen was tested under static intense loads. The reference slab and the slab with a replacement percentage of 20% failed due to flexural failure, whereas the slab with a replacement percentage of 40% failed due to shear failure. The influence of the GFRP replacement ratio was extended to include toughness and ultimate load. A replacement percent of 20% increased them by 18.30, and 2.62%, respectively, while a replacement percent of 40% decreased them by 28.16, and 3.13%, accordingly. It was also shown that the location of replacing the GFRP and 200 mm of unexposed (cold) installation area at the ends with a 45 mm concrete cover has a significant impact. The more the GFRP is located in the middle, away from the ends, the better the fire resistance is.
Date palm fiber is one of the common wastes available in the M. E. countries essentially Iraq. The aim of search to investigate the performance and effects of fiber date palm on the mechanical properties of high strength concrete, this fiber was used in three ratio 2, 4 and 6 % by vol. of concrete at ages of (7, 28, 90) days. Results demonstrated improvement in the compressive strength increased 19.2 %, 23.6%, 24.9 % for 2%, 4%, 6% of fiber respectively at age 28 days. Flexural strength increases 47.6%, 66.2%, 93.8% form (2,4,6) % of fiber respectively at age 28 days. Density increase about 0.41%, 0, 61 % 0.69 % for (2,4,6) % of fiber respectively at age 28. Absorption water decrease
Under-reamed piles defined by having one or more bulbs have the potential for sizeable major sides over conventional straight-sided piles, most of the studies on under-reamed piles have been conducted on the experimental side, while theoretical studies, such as the finite element method, have been mainly confined to conventional straight-sided piles. On the other hand, although several laboratory and experimental studies have been conducted to study the behavior of under-reamed piles, few numerical studies have been carried out to simulate the piles' performance. In addition, there is no research to compare and evaluate the behavior of these piles under dynamic loading. Therefore, this study aimed to numerically investigate bearing capaci
... Show MoreThe behavior of externally prestressed composite beams under short term loading has been studied. A computer program developed originally by Oukaili to evaluate curvature is modified to evaluate the deflection of prestressed composite beam under flexural load. The analysis model based on the deformation compatibility of entire structure that allows to determine the full history of strain and stress distribution along cross section depth, deflection and stress increment in the external tendons .
The evaluation of curvatures for the composite beam involves iterations for computing the strains vectors at each node at any loading stage. The stress increment determined using equations depended on the member deflection at points of connecti
t-Self-Compacting Concrete (SCC) reduces environmental noise and has more workability. This research presents an investigation of the behavior of SCC under mechanical loading (impact loading). Two types of cement have been used to produce SCC mixtures, Ordinary Portland Cement (OPC) and Portland Limestone Cement (PLC), which reduces the emission of carbon dioxide during the manufacturing process. The mixes were reinforced with Carbon Fiber Reinforced Polymer (CFRP) which is usually used to improve the seismic performance of masonry walls, to replace lost steel reinforcements, or to increase column strength and ductility. Workability tests were carried out for fresh SCC. Prepared concrete slabs of 500×500×50mm were tested for lo
... Show MoreComposite steel-concrete sections have a broad benefit through increasing structural strength as well as minimizing the self-loads. All past researches were concerned with pre-installed shear connectors (PRSC) in the manufacturing of composite sections. A new fabrication technique for steel-concrete-steel composite sections were presented in the current study by the post-installation shear connectors (POSC) passed-through an embedded polymerizing vinyl chloride (PVC) pipes. The performance of normal strength concrete prisms with a specified strength of 32 MPa connected to square steel tubes (SST) was investigated. Six specimens were fabricated in both methodologies, PRSC and POSC were experimentally tested by Push-out test. The spac
... Show MoreA theoretical and protection study was conducted of the corrosion behavior of carbon steel surface with different concentrations of the derivative (Quinolin-2-one), namly (1-Amino-4,7-dimethyl-6-nitro-1H-quinolin-2-one (ADNQ2O)). Theoretically, Density Functional Theory (DFT) of B3LYP/ 6-311++G (2d, 2p) level was used to calculate the optimized geometry, physical properties and chemical inhibition parameters, with the local reactivity to predict both the reactive centers and to locate the possible sites of nucleophilic and electrophilic attacks, in vacuum, and in two solvents (DMSO and H2O), all at the equilibrium geometry. Experimentally, the inhibition efficiencies (%IE) in the saline solution (of 3.5%) NaCl were st
... Show More