The microhardness Property of the Biomedical commercially pure titaniumstrontium oxide composite alloy after anodic oxidation
...Show More Authors

Preview PDF
Quick Preview PDF
Publication Date
Sat Feb 01 2025
Journal Name
Journal Of Baghdad College Of Dentistry
The Effect of Pores in Dual Nano Hydroxyapatite Coating on Thermally Oxidized Commercial Pure Titanium: Mechanical and Histological Evaluation
...Show More Authors

Background:In this study,TiO2 layer was thermally grown as a diffusion barrier on CP Ti substrate prior to electrophoretic deposition of HA coatings, to improve the coating’s compatibility also macro and micro pores in nano Hydroxyapatite dual coatings were created and their effect on the bond strength between the bone and implant was evaluated. Materials and methods: Electrophoretic Deposition technique (EPD) was used to obtain coatings for each one of four types of Hydroxyapatite(HA)on CP Ti screws (micro HA, nano HA, dual nano HA with micro pores, dual nano HA with macro pores) where carbon particles used as fugitive material to be removed by thermal treatment to create porosity.For examination of the changes occurred on the subs

... Show More
View Publication Preview PDF
Crossref (2)
Crossref
Publication Date
Fri Apr 01 2022
Journal Name
International Journal Of Early Childhood Special Education
Digital culture skills among chemistry students at the College of Education for Pure Sciences, Ibn al-Haytham in Iraq
...Show More Authors

Preview PDF
Publication Date
Wed May 25 2022
Journal Name
Iraqi Journal Of Science
Transverse Direction Loading Effect on the Elasticity and Strength of Micro and Nano Silica Oxide Composites
...Show More Authors

      Using three-point bending experiments,  the effect of the particle size of SiO2 on the flexural properties of epoxy composites was investigated. Young modulus and flexural strength were studied for different weight percentage of filler  (2,4,6,8 and 10) wt%.The size of SiO2 particles varied from micro (100um) to nano (12nm) .

Flexural strength and  Young modul were found to increase with the filler content, but when the particle size decreased to the nanoscale, the  Young module  increased. Flexural strength was higher for microcomposites than nanocomposites.

View Publication Preview PDF
Scopus (2)
Crossref (1)
Scopus Crossref
Publication Date
Wed Jun 21 2023
Journal Name
Bionanoscience
Evaluation the Antimicrobial Action of Kiwifruit Zinc Oxide Nanoparticles Against Staphylococcus aureus Isolated from Cosmetics Tools
...Show More Authors

View Publication
Scopus (10)
Crossref (6)
Scopus Clarivate Crossref
Publication Date
Sun Jan 01 2017
Journal Name
Proceedings - European Metallurgical Conference, Emc 2017
Friction stir welding of aluminum alloy AA2024-T351 with OFHC copper
...Show More Authors

Scopus
Publication Date
Mon Oct 01 2012
Journal Name
Iraqi Journal Of Physics
Nanostructural study of Ti-Ni binary alloy prepared by mechanical alloying
...Show More Authors

In the present study, a powder mixture of elements Ti and Ni was mechanically alloyed in a high energy ball mill. Microstructure of the nanosized amorphous milled product in different stages of milling has been characterized by X- ray diffraction, scanning electron microscopy and differential thermal analysis. We found that time of mechanical alloying is more significant to convert all crystalline structure to the amorphous phase. Nanocrystalline phase was achieved as a result of the mechanical alloying process. The results also indicates that the phase transformation and the grain size occurs in these alloys are controlled by ball milling time

View Publication Preview PDF
Publication Date
Mon Jun 01 2015
Journal Name
Journal Of Engineering
Mechanical Properties Of AA 6061-T6 Aluminum Alloy Friction Stir Welds
...Show More Authors

The different parameters  on  mechanical  and  microstructural  properties  of  aluminium  alloy  6061-T6 Friction  stir-welded  (FSW) joints  were investigated in the  present study. Different welded  specimens were produced by employing variable rotating  speeds and welding speeds. Tensile strength of the produced joints  was tested at room  temperature and the the effecincy was assessed, it was 75% of the base metal at rotational speed 1500 rpm and weld speed 50 mm/min. Hardness of various zones of FSW welds are presented and  analyzed by  means of  brinell hardness number . Besides to thess tests the bending properties  investigat

... Show More
View Publication Preview PDF
Publication Date
Sat Jul 22 2023
Journal Name
Journal Of Engineering
Investigation Parameters of Resistance Spot Welding For AA1050 Aluminum Alloy Sheets
...Show More Authors

The parameters of resistance spot welding (RSW) performed on low strength commercial aluminum sheets are investigated experimentally, the performance requirements and weldability issues were driven the choice of a specific aluminum alloy that was AA1050. RSW aluminum alloys has a major problem of inconsistent quality from weld to weld comparing with welding steel
alloys sheet, due to the higher thermal conductivity, higher thermal expansion, narrow plastic temperature range, and lower electrical resistivity. Much effort has been devoted to the study of describing the relation between the parameters of the process (welding current, welding time, and electrode force) and weld strength. Shear-tensile strength tests were performed to ind

... Show More
View Publication Preview PDF
Crossref
Publication Date
Sat Dec 30 2017
Journal Name
Al-khwarizmi Engineering Journal
Welding of Low Alloy Steel DIN 15Mo3 by MIG/MAG Spot
...Show More Authors

This research deals with the effects of welding variables using MIG/MAG spot by using Argon (Ar) gas and CO2 to show their effect on the mechanical characteristics and microstructure of low alloy steel type DIN15Mo3 and determine the optimum condition for the process of welding ; current & time. The results show the possibility of using CO2 and also Ar in low alloy steel welding with a little decrease in the shear force of not more than 13% for 4mm thickness and time 2sec. The shear force increased when using Ar instead of CO2 to be , The shear force reach 36KN when using Ar at 2mm thickness  time of 8 sec and current of 220 Amp. , when used CO2 instead of Ar d

... Show More
View Publication Preview PDF
Publication Date
Fri Nov 03 2023
Journal Name
Journal Of Namibian Studies
Consciousness of Green Nanotechnology among Chemistry Scholars at the College of Education for Pure Sciences - Ibn Al-Haitham in Iraq
...Show More Authors

The study's objective is to find out the difference between the scholar of the research sample in awareness Green nanotechnology on the scaleas a whole and in each of its fields. The research depended of (136) specimen mem and women scholars of the fourth stage scholars / Department of Chemistry at the College of Education for Pure Sciences / Ibn Al-Haytham in Iraq for (2022-2023 AD) for the morning and evening studies, (65%) of the scientific community, It was picked at random with relation to the research instrument. it was a measure of awareness of green nanotechnology of (40) items, distributed in three areas (cognitive, skillful, emotional), and its validity and reliability were verified. Data analysis was completed for utilizing the s

... Show More
Preview PDF