High-volume traffic with ultra-heavy axle loads combined with extremely hot weather conditions increases the propagation of rutting in flexible pavement road networks. Several studies suggested using nanomaterials in asphalt modification to delay the deterioration of asphalt pavement. The current work aims to improve the resistance of hot mix asphalt (HMA) to rutting by incorporating Nano Silica (NS) in specific concentrations. NS was blended into asphalt mixtures in concentrations of 2, 4, and 6% by weight of the binder. The behavior of asphalt mixtures subjected to aging was investigated at different stages (short-term and long-term aging). The performance characteristics of the asphalt mixtures were evaluated using the Marshall stability, flow, and wheel tracking tests. Field Emission Scanning Electron Microscopy (FESEM) was utilized to understand the microstructure changes of modified asphalt and estimate the dispersion of NS within the asphalt. The results revealed that using NS–asphalt mixtures as a surface layer in paving construction improved pavement performance by increasing stability, volumetric characteristics, and rutting resistance before and after aging. The FESEM images showed adequate dispersion of NS particles in the mixture. Results indicated that adding 4% of NS to asphalt mixtures effectively enhanced the pavement’s performance and rutting resistance. Doi: 10.28991/CEJ-SP2023-09-01 Full Text: PDF
Moisture damage is described as a reduction in stiffness and strength durability in asphalt mixtures due to moisture. This study investigated the influence of adding nano silica (NS) to the Asphalt on the moisture susceptibility of hot-mix-asphalt (HMA) mixtures under different aging conditions. NS was mixed with asphalt binder at concentrations of 2%, 4%, and 6% by weight of the binder. To detect the microstructure changes of modified Asphalt and estimate the dispersion of NS within the Asphalt, the field emission scanning electron microscope (FE-SEM) was used. To examine the performance of Asphalt mixed with NS at different aging stages (short-term and long-term aging), asphalt mixture tests such as Marshall stability,
... Show MoreOne of the most severe problems with flexible asphalt pavements is permanent deformation in the form of rutting. Accordingly, the practice of adding fiber elements to asphalt mix to improve performance under dynamic loading has grown significantly in order to prevent rutting distress and ensure a safe and long-lasting road surface. This paper explores the effects of a combination of ceramic fiber (CF), a low-cost, easily available mineral fiber, and thermal insulator fiber reinforced to enhance the Marshall properties and increase the rutting resistance of asphalt mixes at high temperatures. Asphalt mixtures with 0%, 0.75%, 1.5%, and 2.25% CF content were prepared, and Marshall stability and wheel tracking tests were employed to stu
... Show MoreRutting is a crucial element of the mechanical performance characteristics of asphalt mixtures, which was the primary target of this study. The task involved substituting various portions of virgin coarse aggregate with recycled concrete aggregate materials that had been treated or left untreated at rates ranging from 25 to 100%, with a constant increase of 25%. The treatment process of recycled concrete aggregate involved soaking in acetic acid, followed by a mechanical process for a short time inside a Los Angeles machine without the balls. This research utilized two primary tests: the standard Marshall test to identify the optimal asphalt contents and the volumetric characteristics of asphalt mixtures. The other one w
... Show MoreThe efforts embedded in this paper have been devoted to designing, preparing, and testing warm mix asphalt (WMA) mixtures and comparing their behavior against traditional hot mix asphalt mixtures. For WMA preparation, the Sasobit wax additive has been added to a 40/50 asphalt binder with a concentration of 3%. An experimental evaluation has been performed by conducting the Marshall together with volumetric properties, indirect tensile strength, and wheel tracking tests to acquire the tensile strength ratio (TSR), retained stability index (RSI), and rut depth. It was found that the gained benefit of reduction in mixing and compaction temperatures was reversely associated with a noticeable decline in Marshall properties and moisture s
... Show MoreRecently, some of Iraq's newly constructed asphalt concrete pavements showed premature failures with significant negative impacts on roadway safety and the economy. Using Nano hydrated lime (NHL) in pavement construction could be one of the possible steps to improve pavement durability. This article discusses how NHL affects the durability of hot mix asphalt. NHL was added in two methods to the asphalt concrete mixture for the wearing course. The first is the dry method, i.e., on the aggregate, whereas the second is the wet addition method, i.e., to the bitumen. The percentages were tried for each additional method; 1, 2, and 3% by weight of aggregate for the dry method and 0.5, 1, and 1.5% by weight of asphalt concrete for the wet
... Show MoreDue to increasing cost of asphalt binder, significant economic savings can be realized by using the amount from reclaimed asphalt pavement (RAP) in the production of new hot mix asphalt (HMA). Moreover, this is an environmentally friendly option as it reduces the demand for virgin materials. It has to be remarked that in Iraq RAP is not used in the production of HMA and this valuable material is mostly degraded for use in lower value applications. Four mixtures were designed, which contains three different percent RAP, it is (0%, 5%, 15%) with asphalt grade (40-50) and (25%) with asphalt grade (60-70), it has been changed the grade of asphalt when adding RAP (25%) to compensate for the aged binder in the RAP when adding to mixture. All type
... Show MorePermanent deformation (Rutting) of asphalt pavements which appears in many roads in Iraq, have caused a major impact on pavement performance by reducing the useful service life of pavement and creating services hazards for highway users. The main objective of this research is investigating the effect of some contributory factors related to permanent deformation of asphalt concrete mixture. To meet the objectives of this research, available local materials are used including asphalt binder, aggregates, mineral filler and modified asphalt binder. The Superpave mix design system was adopted with varying volumetric compositions. The Superpave Gyratory Compactor was used to compact 24 asphalt concrete cylindrical specimens. To collect t
... Show MoreTensile strength is a critical property of Hot Mix Asphalt (HMA) pavements and is closely related to distresses such as fatigue cracking. This study aims to evaluate methods for assessing fatigue cracking in Asphalt Concrete (AC) mixes. In order to achieve optimum density at different binder contents, the mixes were compressed using a gyratory compactor. Tensile strength was assessed using the Indirect Tensile (IDT) and Semi-Circular Bend (SCB) tests. The results showed that the tensile strength measured by the SCB test was consistently higher than that measured by the IDT test at 25 °C. In addition, the SCB test showed a stronger correlation between increasing binder content and tensile strength. For binder contents ranging from 4
... Show More