Structure and Optical Properties of BhSe3 Thin Films Prepared by Chemical Bath Deposition Method
...Show More Authors

Thin films of  BhSe3  have being deposited on glass substrates of

about 80 - 172 ± 14 nm thickness from an aqueous solution bath at temperature 293 K for period 0.5 to 6.0 hours  using alchemical bath deposition method .

The  films  are  characterized   by  X-ray  diffraction,     X-ray

florescent techniques and optical transmittance spectra measurements in the rang 350 - 400 nm at 293 K. And shows that as deposited  films are amorphous and a  transition to polycrystalline state has taken place after  annealing  them  at  373  K,  for  30  minutes,  But  they  will  be dan1aged at 423 K, for the above period. The optical band gab of the films have been found about 1.55 to 1.50 eV as deposited time is increased from 0.5 to 6.0 hours with a  direct allowed type transition.

2 ml. of hydrazine hydrate is added to the aqueous solution bath, the

thickness of the deposited films is found to increase continuously with an increase in dipping period up to 6 hours and it lead to decrease  the deposition time for obtaining a sample of special thickness. Also the magnitude  of  band gap is  decrease  to 1.41-1.38  eV for  the  above periods of time.

View Publication Preview PDF
Quick Preview PDF
Publication Date
Tue Jan 01 2019
Journal Name
Energy Procedia
Evaluation of the optical properties for thick films of epoxy-diamond paste blend prepared by the casting method
...Show More Authors

View Publication
Scopus (2)
Scopus Clarivate Crossref
Publication Date
Mon Apr 24 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Effect of Annealing Temperatures on the Structural and Optical Properties of ZnO and ZnO:Al Thin Films Prepared By Thermal Evaporation Technique
...Show More Authors

 We studied the changing of structural and optical properties of pure and Aluminum-doped ZnO thin films prepared by thermal evaporation technique on glass substrates at thickness (800±50)nm with changing of annealing temperatures ( 200,250,300 )℃ for one hour. The investigation of (XRD) indicates that the pure and doped ZnO thin films were polycrystalline of a hexagonal wurtzite structure with preferred orientation along (002) plane. The grain size was decreased with doping before annealing, but after annealing the grain size is increasing with the increase of annealing temperature for pure film whereas for the doped films with ratios 1 %, 2 % we found that the grain size is larger than that before annealing. The grain size

... Show More
View Publication Preview PDF
Publication Date
Fri Nov 29 2019
Journal Name
Iraqi Journal Of Physics
Morphological and optical properties of V2O5:TiO2 thin film prepared by PLD technique
...Show More Authors

              In this work, pure and doped Vanadium Pentoxide (V2O5) thin films with different concentration of TiO2 (0, 0.1, 0.3, 0.5) wt  were obtained using Pulse laser deposition technique on amorphous glass substrate with thickness of (250)nm. The morphological, UV-Visible and Fourier Transform Infrared Spectroscopy (FT-IR) were studied. TiO2 doping into V2O5 matrix revealed an interesting morphological change from an array of high density pure V2O5 nanorods (~140 nm) to granular structure in TiO2-doped V2O5 thin film .Transform Infrared Spectro

... Show More
View Publication Preview PDF
Crossref (2)
Crossref
Publication Date
Fri Jan 01 2016
Journal Name
Journal Of Multidisciplinary Engineering Science Studies (jmess)
Doping Ratio Of Silver Dependent On The Structure And Optical Properties Of Thin Cadmium Telluride Films
...Show More Authors

Publication Date
Wed Dec 01 2021
Journal Name
Iraqi Journal Of Physics
Effect of Zinc (Zn) -Doped on the Structural, Optical and Electrical Properties of (Cdo)1-Xznx Films Prepared by Pulsed Laser Deposition Technique
...Show More Authors

Pure cadmium oxide films (CdO) and doped with zinc were prepared at different atomic ratios using a pulsed laser deposition technique using an ND-YAG laser from the targets of the pressed powder capsules. X-ray diffraction measurements showed a cubic-shaped of CdO structure. Another phase appeared, especially in high percentages of zinc, corresponding to the hexagonal structure of zinc. The degree of crystallinity, as well as the crystal size, increased with the increase of the zinc ratio for the used targets. The atomic force microscopy measurements showed that increasing the dopant percentage leads to an increase in the size of the nanoparticles, the particle size distribution was irregular and wide, in addition, to increase the surfac

... Show More
View Publication Preview PDF
Crossref
Publication Date
Sun Dec 07 2008
Journal Name
Baghdad Science Journal
Optical Properties for SeTe Thin Films
...Show More Authors

Chalcogenide glasses SeTe have been prepared from the high purity constituent elements .Thin films of SeTe compound have been deposited by thermal evaporation onto glass substrates for different values of film thickness . The effect of varying thickness on the value of the optical gap is reported . The resultant films were in amorphous nature . The transmittance spectra was measured for that films in the wavelength range (400-1100) nm . The energy gap for such films was determined .

View Publication Preview PDF
Crossref
Publication Date
Fri Mar 01 2019
Journal Name
Iraqi Journal Of Physics
Structural and optical properties of Fe- doped ZnO thin films prepared by Sol–Gel spin coating process and their photocatalytic activities
...Show More Authors

Pure and Fe-doped zinc oxide nanocrystalline films were prepared
via a sol–gel method using -
C for 2 h.
The thin films were prepared and characterized by X-ray diffraction
(XRD), atomic force microscopy (AFM), field emission scanning
electron microscopy (FE-SEM) and UV- visible spectroscopy. The
XRD results showed that ZnO has hexagonal wurtzite structure and
the Fe ions were well incorporated into the ZnO structure. As the Fe
level increased from 2 wt% to 8 wt%, the crystallite size reduced in
comparison with the pure ZnO. The transmittance spectra were then
recorded at wavelengths ranging from 300 nm to 1000 nm. The
optical band gap energy of spin-coated films also decreased as Fe
doping concentra

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Fri Jan 01 2021
Journal Name
Aip Conference Proceedings
Optical properties of ZnS and PEDOT thin films
...Show More Authors

Vanadium dioxide nanofilms are one of the most essential materials in electronic applications like smart windows. Therefore, studying and understanding the optical properties of such films is crucial to modify the parameters that control these properties. To this end, this work focuses on investigating the opacity as a function of the energy directed at the nanofilms with different thicknesses(1–100) nm. Effective mediator theories(EMTs), which are considered as the application of Bruggeman’s formalism and the Looyenga mixing rule, have been used to estimate the dielectric constant of VO2 nanofilms. The results show different opacity behaviors at different wavelength ranges(ultraviolet, visible, and infrared). The results depict that th

... Show More
Scopus (2)
Scopus
Publication Date
Tue Jul 01 2014
Journal Name
Journal Of Nanotechnology & Advanced Materials
Structural and optical properties of SnS thin films
...Show More Authors

Thin films of tin sulfide (SnS) were prepared by thermal evaporation technique on glass substrates, with thickness in the range of 100, 200 and 300nm and their physical properties were studied with appropriate techniques. The phase of the synthesized thin films was confirmed by X-ray diffraction analysis. Further, the crystallite size was calculated by Scherer formula and found to increase from 58 to 79 nm with increase of thickness. The obtained results were discussed in view of testing the suitability of SnS film as an absorber for the fabrication of low-cost and non toxic solar cell. For thickness, t=300nm, the films showed orthorhombic OR phase with a strong (111) preferred orientation. The films deposited with thickness < 200nm deviate

... Show More
Publication Date
Thu May 11 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Effect of Annealing Temperature on the Structural and Optical Properties of The CdO Thin Films Prepared By Vacuum Evaporation Thermal Technique
...Show More Authors

      Cadmium Oxide films have been prepared by vacuum evaporation technique on a glass substrate at room temperature. Structural and optical properties of the films are studied at different annealing temperatures (375 and 475) ËšC, for the thickness (450) nm at one hour. The crystal structure of the samples was studied by X- ray diffraction. The highest value of the absorbance is equal to (78%) in the wavelength (530) nm, at annealing temperature (375) ËšC. The value of at a rate of deposition is (10) nm/s. The value of optical energy gap found is equal to (2.22) eV.

View Publication Preview PDF