Ceramic body as a refractory was prepared by using shamoot, which is prepared by firing kaolin Duekhla at 1450 ºC at 2hr ,Flint clay ,Asbestos fiber(Anthophylite type)and Sodium silicts,Phosphoric acid solution as a binder . After miling, siving ,and mixing ,samples were formed, followed that drying, firing at different temperature. Phyical ,thermal and mechanical properties were measured .The conclusion behind the results that the refractory prepared from; 37.5% shamoote,25% Asbestos ,37.5% Flint clay and Phosforic acid solution fired at 1300 ºC gave a refractory material having melting temperature ;1490 ºC, thermal shock resistance 7 cycle, thermal conductivity 2.1w/m2.K, apperant porosity 22.69% ,apperant density 2.87gm/Cm 3 ,Linear shrinkage 3.5%, compressive strength 30.43 MPa and Impact strength 81.3J/Cm2 .
Details
Publication Date
Sun Aug 13 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Volume
22
Issue Number
2
Choose Citation Style
Statistics
View publication
5
Abstract Views
99
Statistics
Preparation of Refractory from local materials
Related publications