Effect of phosphate ester addition on transverse strength and hardness of heat cured acrylic denture base material
...Show More Authors

Background: acrylic resin denture base consider a common denture base material for its acceptable cost, aesthetic and easy processing but still has disadvantages including easy of fracture and low impact strength. Material and method: The experimental group was prepared by addition of 15% phosphoric acid 2-hydroxyethyl methacrylate ester (PA2HEME) with polymethyl methacrylate monomer; the experimental groups was compared with the control one. The specimens were prepared according to ADA specification No. 12 with dimension 65 mm x 10 mm x2.5 mm (length x width x thickness respectively). The prepared specimens were tested by three-point flexural strength utilizing Instron Universal Testing Machine (WDW, Layree Technology Co.), Shore D hardness tester used to measure hardness test. Statistical analysis used student T- test, mean and standard deviation. Results: The result of PA2HEME group showed high significant reduction comparing to the control group for both transverse strength and hardness test. Conclusion: Mixing 15% of PA2HEME with 85% methyl methacrylate (MMA) can reduce the mechanical properties of new modified polymethyl methacrylate (PMMA) acrylic resin.

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Fri Jan 01 2021
Journal Name
Materials Today: Proceedings
Impact of phosphate ester addition on the cytotoxicity of heat cured denture base material
...Show More Authors

This study aims to evaluate and compare the cytotoxicity and biocompatibility of a modified heat-cured acrylic denture base material containing 15% phosphoric acid 2-hydroxyethyl methacrylate ester (PA2HEME) with those of nonmodified PMMA. Discs with a diameter of 12 mm and a thickness of 2 mm were prepared using a heat-cured PMMA denture base material and divided into control and experimental groups. The experimental group was modified with 15% phosphoric acid 2-hydroxyethyl methacrylate ester (PA2HEME). The modified and nonmodified materials were tested via FTIR, and the effect of modification on surface roughness was evaluated with AFM. An in vitro test was conducted to examine the cytotoxicity and biocompatibility of heat-cured acry

... Show More
View Publication
Scopus (1)
Crossref (1)
Scopus Clarivate Crossref
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of plasma treatment of acrylic denture teeth and thermocycling on the bonding strength to heat cured acrylic denture base material
...Show More Authors

Background: Acrylic resin polymer s used in prosthodontic treatment as a denture base material for several decades. Separation and debonding of artificial teeth from denture bases present a laboratory and clinical problem affect patient and dentist. The aim of this study is to evaluate the effect of oxygen plasma and argon plasma treatment of acrylic teeth and thermocycling on bonding strength to hot cured acrylic resin denture base material. Materials and Methods: Sixty denture teeth (right maxillary central incisor) are selected. The denture teeth are waxed onto the beveled surface of rectangular wax block according to Japanese standard for artificial teeth. The control group consisted of 20 denture teeth specimen without any treatment.

... Show More
View Publication Preview PDF
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of addition ZrO2-Al2O3 nanoparticles mixture on some properties and denture base adaptation of heat cured acrylic resin denture base material
...Show More Authors

Background: The PMMA polymer denture base materials are low mechanical properties, adaptation of the denture base to underlying tissue is important for retention and stability of denture. The aim of the study was toevaluate the effect of mixtureZrO2-Al2O3 nanoparticles on impact strength, transverse strength, hardness, roughness, denture base adaptation of heat cured acrylic resin denture base material. Materials and methods: One hundred (100) specimens were prepared, the specimens were divided into five groups (20 specimens to each) according to the test type, each group was subdivided in to two subgroups (control and experimental) each subgroup consist of 10 specimens, the experimental group included mixture of 2% (ZrO2-Al2O3ratio2:1) b

... Show More
View Publication Preview PDF
Publication Date
Mon Nov 05 2018
Journal Name
Iraqi National Journal Of Nursing Specialties
Effect of Addition Retention Bead and Repair Material on Transverse Strength of Repaired Acrylic Denture Resin
...Show More Authors

Objective: One of the most important practical deficiencies of present denture base materials is fracture, therefore many
attempts have been made to reinforce of the repaired denture base resin. A desirable objective for this service is to obtain
optimum strength for repairs, which can be achieved by making available a good bond between original and repaired
materials.
Methodology: The present study was carried out to evaluate and compare the transverse strength of acrylic specimens
repaired by two different materials (hot-cure and cold-cure acrylic resin). A total of 50 specimens were prepared by hot
(40) repair: (10) by hot with retention bead, (10) by cold with retention bead and (10) repair by hot only, (10) repair

... Show More
View Publication Preview PDF
Publication Date
Thu Jun 15 2017
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of modified nanohydroxyapatite fillers addition on some properties of heat cured acrylic denture base materials
...Show More Authors

Background: Poly (methylmethacrylate) is not ideal in every aspect and has disadvantages such as insufficient surface hardness, increase water sorption and poor impact resistance and the latter being the primary cause of fracture of denture base resins. The aim of this study was to evaluate the effect of addition of silanized nano- hydroxyapatite (HA) on some properties of heat cured acrylic denture base material. Materials and methods: HA nano particles were first silanized with MPS (tri methacryloxypropyletrimethoxy silane coupling agent) then ultrasonicated with methylmethacrylate (monomer) to disperse agglomerated nano particles and mixed with polymer. 2% by wt of HA nano particles was selected as the best concentration that add

... Show More
View Publication Preview PDF
Crossref (4)
Crossref
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
The effect of incorporating carbon nanotubes on impact, transverse strength, hardness, and roughness to high impact denture base material
...Show More Authors

Background: One of the most common complications of dentures is its ability to fracture, so the aim of this study was to reinforce the high impact denture base with carbon nanotubes in different concentrations to improve the mechanical and physical properties of the denture base. Materials and methods: Three concentrations of carbon nanotubes was used 0.5%, 1%, 1.5% in a pilot study to see the best values regarding transverse strength, impact, hardness and roughness test, 1 wt% was the best concentration, so new samples for control group and 1wt% carbon nanotubes and the previous tests were of course repeated. Results: There was a significant increase in impact strength and transverse strength when we add carbon nanotubes in 1wt%, compared

... Show More
View Publication Preview PDF
Publication Date
Mon Jan 01 2024
Journal Name
Dental Hypotheses
Effect of Surface Treatments with Plasma and Chemical Bond on Shear Bond Strength of Acrylic Denture Teeth to Flexible and Heat-Cured Denture Base Material: An In Vitro Study
...Show More Authors

Introduction: We aimed to evaluate the shear bond strength of acrylic denture teeth to flexible and heat-cured denture base material after surface treatments with argon plasma, chemical bonding agent (PALFIQUE universal), and combination. Methods: A total of 80 incisor acrylic denture teeth were treated with a argonplasma, chemical bond (PALFIQUE universal bond), and a combination with 10 samples for each group. The neck (gingival portion) of teeth was cut at a 45° angle, and the teeth were attached to heat-cured acrylic resin and flexible denture base material. All the specimens were stored in artificial saliva for 7 days in an incubator (37 °C). A shear

... Show More
View Publication
Scopus Clarivate Crossref
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Evaluation of transverse and tensile bond strength of repaired nylon denture base material by heat, cold and visible light cure acrylic resin
...Show More Authors

Background: Denture fracture is one of the most common problems encountered by the patients and prosthodontists. The objective of present study was to evaluate the transverse strength of nylon denture base resin repaired by using conventional heat polymerized, autopolymerized and visible light cure {VLC} resins, surface treatment that used for repair and adjustment of insufficient nylon denture bases and in case of addition of artificial teeth. As these corrective procedures are common chair side procedures in dental clinic. Materials and methods: One hundred twenty nylon specimens were prepared by using metal patterns with dimension of (65x10x2.5 mm) length, width, and thickness respectively for transverse strength test while for tensile b

... Show More
View Publication Preview PDF
Publication Date
Mon Mar 13 2017
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of The CO2 Laser as Surface Treatment on The Bond Strength of Heat Cured Soft Liner to The High Impact Acrylic Denture Base Material
...Show More Authors

ABSRTACT Background: Soft liner material is become important in dental prosthetic treatment. They are applied to the surface of the dentures to achieve more equal force distribution , reduce localized pressure and improve denture retention by engaging undercut . So the aim of the study is to evaluate the effect of different surface treatment by air-abrasion AL2O3 and laser treatment with CO2 laser on improving the shear bond strength of the denture liner to acrylic denture base material . Materials and methods: the 30 specimens of heat cured acrylic denture base material (high Impact acrylic )and heat cured soft liner (Vertex ,Nether Lands )were prepared for this study .They were designed and divided according to type of the s

... Show More
View Publication Preview PDF
Crossref (5)
Crossref
Publication Date
Thu Dec 19 2024
Journal Name
Journal Of Baghdad College Of Dentistry
The effect of addition nano particle ZrO2 on some properties of autoclave processed heat cure acrylic denture base material
...Show More Authors

Background: Polymethyl methacrylate (PMMA) is used in denture fabrication and considered as the most reliable material for the construction of removable prosthodontic appliances. The material is far from ideal in fulfilling the mechanical requirements and the effect of autoclave processing has not been fully determined. The purpose of this study was to evaluate the effect of addition of salinized (ZrO2) Nano fillers in percentages 3%, 5% and 7% by weight on some properties of heat cured acrylic processed the by autoclave and compare it with 0% (control) group . Materials and methods: The silanized(ZrO2) Nano-particles was added to PMMA powder by weight in three different percentages 3%, 5% and 7%, mixed by probe ultra-sonication machine.

... Show More
View Publication Preview PDF