By extracting crystal violate dye (CV) from its aqueous solution, the photocatalytic decolorization performance of ZnO/MWCNT nanocomposite was evaluated. The nanocomposite was prepared by precipitation of ZnO and incorporates on the surface of Multi-Walled Carbon Nanotubes (MWCNT). ZnO nanoparticles were synthesized using the sol gel process with MWCNT acting as a template. They were then analyzed by XRD, SEM, and TEM, which revealed how the shape of the spherical nano ZnO interacts with the point of zero charge (pzc), which allows us to see the physical attributes. In the dipping photoreactor, which included a slurry of dye solution and ZnO/MWCNT nanocomposite, the effectiveness of decolorization was assessed. The photodecolorization was studied for CV dye in aqueous solution at different conditions: The effect of time, weight of catalyst, concentration of dye, temperature, the initial pH of dye solution and addition of S2O82- to show the optimum condition of this process. The main results were the synthesis of incorporated ZnO on MWCNT surface with 10-20 nm with high photodecolorization against CV dye. Full decolorization reached at 90 min and 89.8% decolorization at the half time of reaction. ZnO/MWCNT weight of 0.06 gm per 100 mL was optimum for photodecolorization. The photocatalytic reaction was more efficient in the deceasing of CV concentration and obeys the Langmuir-Hinshelwood kinetic, while the photodecolorization was not less than 95% in pH range 6-10.Also, the photocatalytic reaction was effected in the presence of S2O82-, where the photodecolorization was more efficient.
The object of this study was to evaluate the efficiency of safranin O (SFO), dye removal with application of Thuja orientalis as a low-cost biosorbent. The biosorption equilibrium level was determined as a function of pH, adsorbent dose, contact time and temperature. Surface area and pore size distribution were measured for the adsorbent. Thuja has a good removal effeciency for SFO dye. The adsorption kinetics data were best fit for the pseudo-second order kinetic (the regression coefficient = 0.999). The experimental equilibrium adsorption data are tested for the Langmuir, freundlich,Temkin and Dubinin-Radushkevich isotherm modles. From the values of the regression coefficient the results indicate the following order to fit the isotherm
... Show MoreThere is currently a pressing need to create an electro-analytical approach capable of detecting and monitoring genosensors in a highly sensitive, specific, and selective way. In this work, Functionalized Multiwall Carbon Nanotubes, Graphene, Polypyrrole, and gold nanoparticles nanocomposite (f-MWCNTs-GR-PPy-AuNP) were effectively deposited on the surface of the ITO electrode using a drop-casting process to modify it. The structural, morphological, and optical analysis of the modified ITO electrodes was carried out at room temperature using X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM) images, atomic force microscopy (AFM) and Fourier transform infrared (FTIR) spectra. Cyclic voltammetry (CV) and electrochemi
... Show MoreThe reactive yellow azo dye (λmax = 420 nm) is widely utilized for textile coloring due to its low-cost stability and tolerance properties. Treatment of dye-containing wastewater by traditional methods is usually inadequate because of its resistance to biological and chemical degradation. From this research, the continuous reactor of an advanced oxidation method supported the use of H2O2/TiO2/UV to remove the coloration of the reactive yellow dye from the discharge. At constant best conditions obtained from the batch reactor tests pH=7, H2O2 dosage = 400 mg/l and TiO2=25mg/l , the aqueous solutions were tested in the continuous reactor at different dye concentration and d
... Show MoreAbstract This study investigated the treatment of textile wastewater contaminated with Acid Black 210 dye (AB210) using zinc oxide nanoparticles (ZnO NPs) through adsorption and photocatalytic techniques. ZnO NPs were synthesized using a green synthesis process involving eucalyptus leaves as reducing and capping agents. The synthesized ZnO NPs were characterized using UV-Vis spectroscopy, SEM, EDAX, XRD, BET, Zeta potential, and FTIR techniques. The BET analysis revealed a specific surface area and total pore volume of 26.318 m2/g. SEM images confirmed the crystalline and spherical nature of the particles, with a particle size of 73.4 nm. A photoreactor was designed to facilitate the photo-degradation process. The study investigated the inf
... Show MorePhotocatalytic degradation of methylene blue was studied using CdS and ZnS as catalyst. The photocatalytic activity of the specimen was studied by exposing to UV-radiation. The result shows that the degradation efficiency of the dye for CdS micro-particles was 92% after 7 hours and for ZnS micro-particles was 88.29% for the same time interval.
Electrochemical decolorization of direct black textile dye was studied in the presence of sodiumhydroxide (NaCl). Electrochemical cell occupy about 1 liter of working electrolyte supplied with graphiteelectrodes for both anode and cathode was constructed for this purpose. Decolorization percent, treatment time, power consumption, and pH were studied as a function of the applied voltage and salt concentration. Results show that decolorization increase with increasing salt concentration and applied voltage. Best decolorization of 86% can be achieved after 17 min at 7 volt and 5 g/l salt concentration. Further decolorization can be achieved but this will be accompanied with a sharp increase in power consumption. No significant decrease
... Show MoreIn this work, the photocatalytic degradation of indigo carmine (IC) using zinc oxide suspension was studied. The effect of influential parameters such as initial indigo carmine concentration and catalyst loading were studied with the effect of Vis irradiation in the presence of reused ZnO was also investigated. The increased in initial dye concentration decreased the photodegradation and the increased catalyst loading increased the degradation percentage and the reused-ZnO exhibits lower photocatalytic activity than the ZnO catalyst. It has been found that the photocatalytic degradation of indigo carmine obeyed the pseudo-first-order kinetic reaction in presence of zinc oxide. This was found from plotting the relationship between ln
... Show MoreThe solar photocatalytic degradation of diuron, which is one of the herbicides, has been studied by a solar pilot plant in heterogeneous solar photocatalysis with titanium dioxide. The pilot plant was made up of compound parabolic collectors specially designed for solar photocatalytic applications. The influence of different variables such as, H2O2 initial concentration, TiO2 initial concentration, and diuron initial concentration with their relationship to the degradation efficiency were studied. Hydrogen peroxide (H2O2) found to increase the rate of diuron degradation. The best removal efficiency of heterogeneous solar photocatalytic TiO2 system was found to be 46.65 % and for heterogeneous solar photocatalytic TiO2/ H2O2 system was fo
... Show MoreIn this work, zinc oxide nanoparticles (ZnONPs) and sawdust/epoxy composite (20:80) were mixed using a simple molding method with different ZnONPs concentrations of (0.1, 0.3, 0.5, 0.7, and 1.0 %). The samples of the nanocomposites were characterized by the Scanning Electron Microscopy (SEM) technique to demonstrate the homogeneity of the prepared ZnONPs/nanocomposites. The photocatalytic activity of the samples was examined using the methylene blue (MB) dye as a pollutant solution, through evaluation of the efficiency of the prepared compound in the treatment of organic pollutants under illumination by sunlight. The photocatalytic results showed that after 240 minutes of exposure to sunlight, the sample prepared using (0.5 vol.% of ZnON
... Show MoreThe present research was conducted to synthesis Y-Zeolite by sol-gel technique using MWCNT (multiwalled carbon nanotubes) as crystallization medium to get a narrow range of particle size distribution with small average size compared with ordinary methods. The phase pattern, chemical structure, particle size, and surface area were detected by XRD, FTIR, BET and AFM, respectively. Results shown that the average size of Zeolite with and without using MWCNT were (92.39) nm and (55.17) nm respectively .Particle size range reduced from (150-55) nm to (130-30) nm. The surface area enhanced to be (558) m2/g with slightly large pore volume (0.231) km3/g was obtained. Meanwhile, degree of crystallization decrease
... Show More