Preferred Language
Articles
/
ijs-6031
Effect of Additives on Impact Strength of Denture Base Resin
...Show More Authors

This research has studied the effect of addition glass fibers (woven and chopped)
and Zirconium oxide Nano-particles (ZrO2) with different weight percent to the
conventional poly (methyl methacrylate) (PMMA). The prepared Nano-crystalline
ZrO2 powder with particle size of about 95nm was syntheses directly by sol-gel
method. The gel dried at 100oC for 1 hour and annelid at 400oC for 3 hours.
The conventional acrylic resin prepared with 2:1 powder to liquid ratio to prepare
pure sample, composite samples prepared by reinforcing PMMA with woven or
chopped glass fiber (8, 12) wt.%, and reinforcing by (1,2,3) wt.% of prepared ZrO2
Nano-powder.
The structural tests include: (XRD, AFM, and FTIR). The crystallized phase
composition of dried ZrO2 powder after annealing in air at 400oC has been identified
by x-ray diffractometry (XRD). The grain size of dried ZrO2 Nano-particles by
atomic force microscope (AFM).
The impact strength (I.S.) was measured by using Charpy impact test. The
mechanical test done in order to compare the impact strength between pure and
composite samples. From the result, the reinforcing PMMA with glass fiber in two
forms (woven and chopped) improve the impact strength, while increasing of ZrO2
Nano powder loading led to decrease the impact strength.

View Publication Preview PDF
Quick Preview PDF
Publication Date
Sun Mar 01 2020
Journal Name
Iraqi Journal Of Physics
Studying the Impact Strength of Layered Denture Base Resin
...Show More Authors

This paper displays the effect of uncoated and coated chopped carbon fibers with alumina Al2O3 or Tri calcium phosphate (TCP) on the impact strength of acrylic poly methyl methacrylate (PMMA) denture base resin. To improve bonding between carbon fibers and coating materials powders, the surface of carbon fibers has been treated with Para amino benzoic acid (C9H10N2O3) and poly vinyl alcohol (PVA) was also used. The morphology of the coating layers has been examined by field emission scanning electron microscope (FE-SEM). From the results, PMMA reinforced with uncoated chopped carbon fiber has high impact strength value but still have bad aesthetic.  Samples prepared b

... Show More
View Publication Preview PDF
Crossref (4)
Crossref
Publication Date
Wed Nov 07 2018
Journal Name
Iraqi National Journal Of Nursing Specialties
Effect of metal wire and glass fibers on the impact strength of acrylic denture-base resin
...Show More Authors

Objective(s): The aim of this study is to compare the impact strength of a heat cured denture-base acrylic resin
reinforced with metal wire and glass fibers.

Methodology: Forty five specimens were prepared from pink heat cure acrylic resin. Specimens were grouped into;
group-I (control group) which consists of 15 specimens with no reinforcement, group-II which consists of 15 specimens
reinforced with metal wire, and group-III consists of 15 specimens reinforced with glass fibers. Specimens were tested
by using charpy impact machine.

Results: The result showed that there was a highly significant difference in impact strength value among the testing
groups at (P < 0.001).

Conclusion: The impact str

... Show More
View Publication Preview PDF
Publication Date
Sun Oct 01 2023
Journal Name
Nanomedicine Research Journal
The effect of ZrO2 NPs addition on denture adaptation and diametral compressive strength of 3D printed denture base resin
...Show More Authors

Objective(s): The world of dentistry is constantly evolving, and with the advent of 3D printing technology, the possibilities are endless. However, little is known about the effects of adding ZrO2 NPs to the denture base resin of 3D additive manufacturing technique.Aim of this study is to evaluate the behavior of resin which is used to 3D printing of denture base with the addition of ZrO2 NPs on denture adaptation property and diametral compression strength.Methods: 60 samples were printed, 30 disks for diametral compressive test and 30 denture base for denture adaptation test. Three groups per test (n=10). The control group for each test included unreinforced 3Dprinted denture base resin, and the other groups were  reinforced with (2&

... Show More
View Publication
Publication Date
Mon Dec 23 2024
Journal Name
Journal Of Baghdad College Of Dentistry
The effect of incorporating carbon nanotubes on impact, transverse strength, hardness, and roughness to high impact denture base material
...Show More Authors

Background: One of the most common complications of dentures is its ability to fracture, so the aim of this study was to reinforce the high impact denture base with carbon nanotubes in different concentrations to improve the mechanical and physical properties of the denture base. Materials and methods: Three concentrations of carbon nanotubes was used 0.5%, 1%, 1.5% in a pilot study to see the best values regarding transverse strength, impact, hardness and roughness test, 1 wt% was the best concentration, so new samples for control group and 1wt% carbon nanotubes and the previous tests were of course repeated. Results: There was a significant increase in impact strength and transverse strength when we add carbon nanotubes in 1wt%, compared

... Show More
View Publication Preview PDF
Publication Date
Mon Dec 23 2024
Journal Name
Journal Of Baghdad College Of Dentistry
The Effect of Plasma Treatment on Shear Bond Strength of High Impact Acrylic Resin Denture Base Lined with Two Types of Soft Lining Materials after Immersion in Distilled Water and Denture Cleanser
...Show More Authors

Background: In dentistry, dentist takes the advantages of soft lining materials due to the viscoelastic properties. The major problem is the adhesion of the soft liner with the denture base material. Materials and Methods: Heat cured of high impact acrylic resin specimens prepared with dimensions 75x13x13mm for shear bond strength test, soft lining material (Refit and Mollosil) with a 3-mm thickness and used to join each two acrylic blocks. Also four specimens with the same previous dimensions utilized for chemical and physical surface analysis. The specimens grouped as control (without plasma) and experiment (with oxygen plasma) treated high impact acrylic specimens. Results: Plasma treatment increased the shear bond strength for both Refi

... Show More
View Publication Preview PDF
Publication Date
Mon Nov 05 2018
Journal Name
Iraqi National Journal Of Nursing Specialties
Effect of Mechanical Surface Treatment on the Tensile Bond Strength of Repaired Acrylic Denture Base Resin Cured by Two Different Techniques
...Show More Authors

Objective: To evaluate and compare the effect of mechanical surface treatment (groove, aluminum oxide particles)
with 45 degree bevel type of joint on tensile bond strength of acrylic specimens repaired by two curing methods
(microwave and water both).
Methodology: Eighty specimens (80) were prepared from pink heat cure acrylic resin. They were divided into two
main groups (40 specimen repaired by microwave energy and 40 specimens repaired by water bath method).Each
group can be divided into four subgroups of ten according to the surface treatment. The control group A was left
intact, group B received no surface treatment, group C and D received surface treatment by (groove, 50 m aluminum
oxide particles). Specimens

... Show More
View Publication Preview PDF
Publication Date
Mon Dec 23 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of addition ZrO2-Al2O3 nanoparticles mixture on some properties and denture base adaptation of heat cured acrylic resin denture base material
...Show More Authors

Background: The PMMA polymer denture base materials are low mechanical properties, adaptation of the denture base to underlying tissue is important for retention and stability of denture. The aim of the study was toevaluate the effect of mixtureZrO2-Al2O3 nanoparticles on impact strength, transverse strength, hardness, roughness, denture base adaptation of heat cured acrylic resin denture base material. Materials and methods: One hundred (100) specimens were prepared, the specimens were divided into five groups (20 specimens to each) according to the test type, each group was subdivided in to two subgroups (control and experimental) each subgroup consist of 10 specimens, the experimental group included mixture of 2% (ZrO2-Al2O3ratio2:1) b

... Show More
View Publication Preview PDF
Publication Date
Wed Dec 14 2016
Journal Name
Journal Of Baghdad College Of Dentistry
Evaluation of Impact and Transverse Strength of Denture Bases Repaired with Nano Reinforced Resin
...Show More Authors

Background: Failure of resin bases were a major disadvantage recorded in the constructed dentures. Reinforcements of the repair joint with nano fillers represent an attempt to enhance the strength and durability. The purpose of the research was to estimate the influence of nano fillers reinforcement with (ZrO2 and Al2O3) on impact and transverse strength of denture bases repaired with either cold or hot processing acrylic resin. Materials and methods: A hundred and forty (140) samples were processed with hot cured resin and organized in subgroups depending on the repair materials and condition (without repair (control), repair with hot cure, cold cure, hot and cold cure reinforced with either (5% Zr2O or 0.5% Al2O3). The samples in these

... Show More
View Publication Preview PDF
Crossref
Publication Date
Tue Dec 01 2009
Journal Name
Iraqi Journal Of Physics
Effect of Polyurethane Resin Additives on the Impact Toughness of Epoxy Resin Reinforced with woven roving Glass
...Show More Authors

I mpact strength for Epoxy/Polyurethane, Blends and their composites with two
layers of Glass fibers (0-90) are calculated.
The impact strength of the blends and composites decrease with increasing weight
by weisht percentage of polyurethane . This result is attributed to the high elasticity
of PU , and to the immiscibility between the polymer blends as well as the fiber
delaminates

View Publication Preview PDF
Publication Date
Mon Nov 05 2018
Journal Name
Iraqi National Journal Of Nursing Specialties
Effect of Addition Retention Bead and Repair Material on Transverse Strength of Repaired Acrylic Denture Resin
...Show More Authors

Objective: One of the most important practical deficiencies of present denture base materials is fracture, therefore many
attempts have been made to reinforce of the repaired denture base resin. A desirable objective for this service is to obtain
optimum strength for repairs, which can be achieved by making available a good bond between original and repaired
materials.
Methodology: The present study was carried out to evaluate and compare the transverse strength of acrylic specimens
repaired by two different materials (hot-cure and cold-cure acrylic resin). A total of 50 specimens were prepared by hot
(40) repair: (10) by hot with retention bead, (10) by cold with retention bead and (10) repair by hot only, (10) repair

... Show More
View Publication Preview PDF