Compressive Strength Performance of Reactive Powder Concrete Using Different Types of Materials as a Partial Replacement of Fine Aggregate
...Show More Authors

Reactive Powder Concrete (RPC) can be incorporate as a one of the most important and progressive concrete technology. It is a special type of ultra-high strength concrete (UHSC) that’s exclude the coarse aggregate from its constitutive materials. In this research an experimental study had been carried out to investigate the effect of using three types of materials (porcelain aggregate) and others sustainable materials (glass waste and granular activated carbon) as a partial replacement of fine aggregate. Four percentages had considered (0, 10, 15 and 20) % to achieve better understanding for the influence of these materials upon the compressive strength of RPC. Four curing ages had included in this study, these are; 7, 28, 60 and 90 days. The outcomes of the experimental works improved that using porcelain aggregate as a partial replacement had an advanced effect on the compressive strength for all the adopted percentages and for all the studied curing ages. The maximum modification that’s obtained in case of porcelain aggregate was (24.14) % at age (90) days for 20% replacement. Using glass waste caused an increase in the overall values of the compressive strength for all the adopted replacements with less efficient than porcelain to reached (20.69) % at age (90) days for 20% replacement. Regarding the granular activated carbon, only (10%) replacement had a positive influence on the compressive strength to reached (13.16) % while the others caused a reduction in the compressive strength reached to (29.13)% for 20% replacement.

Crossref
View Publication